Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.829 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.054 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.14 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToHCl |
Band Gap5.181 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImm2 [44] |
HallI 2 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 183.8 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 277.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 129.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 110.8 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 122.2 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 217.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 147.7 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 317.7 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 166.2 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 97.7 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 139.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 184.6 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 153.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 147.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 313.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 341.6 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 199.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 110.8 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 183.8 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 147.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 122.2 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 214.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 195.5 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 1> | 275.6 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 195.5 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 97.7 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 139.7 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 314.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 166.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 217.4 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 146.6 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 129.3 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 158.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 166.2 |
KCl (mp-23193) | <1 1 0> | <1 1 1> | 118.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 166.2 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 171.0 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 91.9 |
Te2W (mp-22693) | <1 0 0> | <1 1 1> | 197.6 |
Te2W (mp-22693) | <1 1 0> | <1 0 1> | 217.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 221.6 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 139.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 171.0 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 183.8 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 104.8 |
YVO4 (mp-19133) | <0 0 1> | <0 1 1> | 153.1 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 91.9 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 214.4 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 249.7 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 139.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.17073 | -0.00187 | -0.01364 | 0.00000 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.01412 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.01144 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.17128 C/m2 |
Crystallographic Direction vmax |
---|
1.00000 |
0.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
1.88 | 0.00 | 0.00 |
0.00 | 1.81 | 0.00 |
0.00 | 0.00 | 1.80 |
Dielectric Tensor εij (total) |
||
---|---|---|
1.89 | 0.00 | 0.00 |
0.00 | 1.81 | 0.00 |
0.00 | 0.00 | 1.80 |
Polycrystalline dielectric constant
εpoly∞
1.83
|
Polycrystalline dielectric constant
εpoly
1.83
|
Refractive Index n1.35 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HBr (mp-32684) | 0.6405 | 0.023 | 2 |
HI (mp-697025) | 0.7185 | 0.000 | 2 |
SN (mp-1078816) | 0.6041 | 0.690 | 2 |
NO (mp-31000) | 0.7246 | 0.467 | 2 |
H2 (mp-632172) | 0.3021 | 0.000 | 1 |
F2 (mp-561367) | 0.7068 | 0.000 | 1 |
H2 (mp-850274) | 0.6818 | 0.000 | 1 |
O2 (mp-1009490) | 0.7481 | 0.002 | 1 |
O2 (mp-1087546) | 0.6815 | 0.202 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: H Cl |
Final Energy/Atom-3.0758 eV |
Corrected Energy-6.1515 eV
-6.1515 eV = -6.1515 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)