Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.535 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.117 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.54 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBi2O3 |
Band Gap0.969 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 306.7 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 213.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 306.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 200.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 226.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 213.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 146.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 200.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 266.7 |
GaAs (mp-2534) | <1 0 0> | <1 -1 -1> | 168.3 |
GaAs (mp-2534) | <1 1 1> | <1 -1 -1> | 168.3 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 213.4 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 226.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 293.4 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 333.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 200.0 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 230.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 173.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 173.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 106.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 173.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 133.4 |
GaN (mp-804) | <1 1 1> | <1 -1 0> | 250.7 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 93.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 293.4 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 157.5 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 236.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 253.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 226.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 280.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 186.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 160.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 306.7 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 333.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 226.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 93.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 200.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 146.7 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 160.0 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 253.4 |
ZnSe (mp-1190) | <1 0 0> | <1 -1 -1> | 168.3 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 226.7 |
ZnSe (mp-1190) | <1 1 1> | <1 -1 -1> | 168.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 160.0 |
CdS (mp-672) | <1 0 0> | <1 -1 -1> | 84.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 200.0 |
LiF (mp-1138) | <1 0 0> | <1 -1 -1> | 84.1 |
LiF (mp-1138) | <1 1 0> | <1 -1 -1> | 168.3 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 333.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 160.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Explore more synthesis descriptions for materials of composition Bi2O3.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Bi O |
Final Energy/Atom-5.6368 eV |
Corrected Energy-90.7354 eV
Uncorrected energy = -84.5524 eV
Composition-based energy adjustment (-0.687 eV/atom x 9.0 atoms) = -6.1830 eV
Corrected energy = -90.7354 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)