Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-1.510 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.166 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.26 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToYbSe + Se |
Band Gap0.792 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI42d [122] |
HallI 4 2bw |
Point Group42m |
Crystal Systemtetragonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 77.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 311.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 77.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 155.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 233.3 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 233.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 311.1 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 233.3 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 311.1 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 233.3 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 155.5 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 311.1 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 311.1 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 311.1 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 77.8 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 311.1 |
Au (mp-81) | <1 0 0> | <0 0 1> | 155.5 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 77.8 |
CaCO3 (mp-3953) | <1 1 0> | <0 0 1> | 155.5 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <0 0 1> | 155.5 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 311.1 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 233.3 |
MgF2 (mp-1249) | <1 1 1> | <0 0 1> | 233.3 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 77.8 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 77.8 |
SrTiO3 (mp-4651) | <0 0 1> | <0 0 1> | 155.5 |
SrTiO3 (mp-4651) | <1 1 0> | <0 0 1> | 311.1 |
CaF2 (mp-2741) | <1 0 0> | <0 0 1> | 155.5 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 233.3 |
ZnTe (mp-2176) | <1 0 0> | <0 0 1> | 77.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SbF4 (mvc-15178) | 0.4905 | 0.181 | 2 |
Np2Se3 (mp-684922) | 0.4965 | 0.000 | 2 |
Ce2Te3 (mp-32838) | 0.4920 | 0.000 | 2 |
U2Te3 (mp-684787) | 0.4518 | 0.000 | 2 |
Yb2S3 (mp-684680) | 0.1815 | 0.113 | 2 |
Na3TaF8 (mp-17245) | 0.5235 | 0.000 | 3 |
Y4OsBr4 (mp-28744) | 0.5484 | 0.000 | 3 |
La10US16 (mp-675741) | 0.5299 | 0.051 | 3 |
Nb(SeCl)2 (mp-27361) | 0.5446 | 0.008 | 3 |
CeCu4Sn (mp-655580) | 0.5040 | 0.298 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points10 |
U Values-- |
PseudopotentialsVASP PAW: Yb_2 Se |
Final Energy/Atom-4.2149 eV |
Corrected Energy-168.5952 eV
-168.5952 eV = -168.5952 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)