Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.614 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.037 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.75 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBi2O3 |
Band Gap1.686 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 230.2 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 230.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 153.5 |
Te2W (mp-22693) | <1 1 0> | <0 0 1> | 230.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 230.2 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 230.2 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 230.2 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 230.2 |
C (mp-66) | <1 1 0> | <0 0 1> | 307.0 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 230.2 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 230.2 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 230.2 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <0 0 1> | 153.5 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 153.5 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 153.5 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 230.2 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 307.0 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 230.2 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 76.7 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 230.2 |
YAlO3 (mp-3792) | <1 1 1> | <0 0 1> | 307.0 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 230.2 |
ZrO2 (mp-2858) | <1 0 1> | <0 0 1> | 307.0 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <0 0 1> | 153.5 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 230.2 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 307.0 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 307.0 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 230.2 |
GaSb (mp-1156) | <1 1 0> | <0 0 1> | 230.2 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 230.2 |
LiAlO2 (mp-3427) | <1 0 1> | <0 0 1> | 307.0 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 230.2 |
ZnTe (mp-2176) | <1 1 0> | <0 0 1> | 153.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
FeBi25O39 (mp-698573) | 0.5248 | 0.027 | 3 |
GaBi25O39 (mp-849761) | 0.4484 | 0.021 | 3 |
FeBi25O39 (mp-761437) | 0.4255 | 0.025 | 3 |
TlBi25O39 (mp-531130) | 0.2070 | 0.025 | 3 |
Zn(Bi19O30)2 (mp-685869) | 0.4773 | 0.040 | 3 |
Zn2NiWO6 (mvc-6767) | 0.7364 | 0.176 | 4 |
Bi25O38 (mp-766354) | 0.3082 | 0.042 | 2 |
Bi19O30 (mp-773884) | 0.5779 | 0.050 | 2 |
Bi2O3 (mp-759526) | 0.2815 | 0.034 | 2 |
Explore more synthesis descriptions for materials of composition Bi2O3.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Bi O |
Final Energy/Atom-5.7169 eV |
Corrected Energy-982.1259 eV
-982.1259 eV = -914.7061 eV (uncorrected energy) - 67.4198 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)