Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.079 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.291 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.94 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa2SiO4 + NaF |
Band Gap2.583 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <1 0 1> | 255.7 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 172.3 |
AlN (mp-661) | <1 1 0> | <1 -1 -1> | 109.3 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 126.9 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 317.3 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 84.5 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 258.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 317.3 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 169.1 |
GaN (mp-804) | <1 0 1> | <0 1 -1> | 262.5 |
GaN (mp-804) | <1 0 0> | <1 1 1> | 102.0 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 59.8 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 299.2 |
SiO2 (mp-6930) | <1 1 1> | <0 1 -1> | 262.5 |
SiO2 (mp-6930) | <1 0 0> | <1 -1 -1> | 109.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 179.5 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 169.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 253.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 -1 -1> | 109.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 -1 -1> | 109.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 253.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 85.2 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 258.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 255.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 255.7 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 317.3 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 255.7 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 239.3 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 255.7 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 255.7 |
YVO4 (mp-19133) | <1 0 1> | <1 0 -1> | 267.5 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 170.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 299.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 253.8 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 253.6 |
BN (mp-984) | <1 0 1> | <1 0 0> | 317.3 |
BN (mp-984) | <1 1 1> | <1 0 1> | 170.5 |
BN (mp-984) | <0 0 1> | <0 1 0> | 185.4 |
BN (mp-984) | <1 0 0> | <0 1 0> | 247.2 |
BN (mp-984) | <1 1 0> | <0 1 1> | 169.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 253.8 |
Al (mp-134) | <1 0 0> | <1 1 0> | 258.5 |
Al (mp-134) | <1 1 0> | <1 0 1> | 255.7 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 1> | 253.6 |
LiGaO2 (mp-5854) | <0 0 1> | <1 -1 -1> | 109.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 0> | 258.5 |
LiGaO2 (mp-5854) | <1 0 1> | <1 1 0> | 86.2 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 255.7 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 63.5 |
SiC (mp-7631) | <0 0 1> | <1 -1 0> | 90.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca4Al3O10 (mp-675084) | 0.6168 | 0.480 | 3 |
Ba4Y2O7 (mp-779544) | 0.7458 | 0.099 | 3 |
Mn4(PO4)3 (mp-540071) | 0.7454 | 0.035 | 3 |
Nb10Pb14O39 (mp-707290) | 0.6921 | 0.096 | 3 |
LiCu4(PO4)3 (mp-673145) | 0.6948 | 0.062 | 4 |
Li3Fe(PO4)2 (mp-761558) | 0.5864 | 0.278 | 4 |
LiCrPO4 (mp-761398) | 0.6943 | 0.045 | 4 |
NaCuAsO4 (mp-559209) | 0.6451 | 0.031 | 4 |
Na3Ga(PO4)2 (mp-561058) | 0.5807 | 0.000 | 4 |
Na2Li2V3P2O13 (mp-853239) | 0.6949 | 0.061 | 5 |
NaLiMo(H2O3)2 (mp-540983) | 0.6622 | 0.013 | 5 |
KNaCu3S3O13 (mp-554726) | 0.7206 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Ca_sv Si O F |
Final Energy/Atom-6.3162 eV |
Corrected Energy-240.2245 eV
Uncorrected energy = -227.3845 eV
Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV
Composition-based energy adjustment (-0.462 eV/atom x 4.0 atoms) = -1.8480 eV
Corrected energy = -240.2245 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)