Final Magnetic Moment38.466 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.159 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.046 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.44 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe3N + FeN |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 282.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 181.3 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 197.1 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 181.3 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 94.3 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 154.3 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 122.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 282.8 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 197.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 282.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 122.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 282.8 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 282.8 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 282.8 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 1> | 181.3 |
Si (mp-149) | <1 0 0> | <1 0 1> | 181.3 |
CdSe (mp-2691) | <1 0 0> | <0 1 1> | 154.3 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 282.8 |
WS2 (mp-224) | <1 1 0> | <1 0 0> | 154.7 |
MgO (mp-1265) | <1 1 0> | <0 1 1> | 154.3 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 154.7 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 282.8 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 282.8 |
ZrO2 (mp-2858) | <1 1 0> | <0 1 0> | 122.2 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 282.8 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 282.8 |
Mg (mp-153) | <1 1 1> | <1 0 1> | 181.3 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 282.8 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 154.7 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 154.7 |
PbS (mp-21276) | <1 1 0> | <0 1 1> | 154.3 |
SiC (mp-8062) | <1 0 0> | <0 1 1> | 154.3 |
GaP (mp-2490) | <1 0 0> | <1 0 1> | 181.3 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 282.8 |
InP (mp-20351) | <1 1 0> | <0 1 1> | 154.3 |
Ni (mp-23) | <1 0 0> | <1 1 0> | 197.1 |
MgF2 (mp-1249) | <0 0 1> | <1 1 0> | 197.1 |
PbSe (mp-2201) | <1 0 0> | <0 1 1> | 154.3 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 282.8 |
GaSb (mp-1156) | <1 0 0> | <0 1 1> | 154.3 |
GaTe (mp-542812) | <1 0 0> | <1 0 1> | 181.3 |
CaF2 (mp-2741) | <1 0 0> | <1 0 1> | 181.3 |
ZnTe (mp-2176) | <1 0 0> | <0 1 1> | 154.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Al(BiO3)3 (mvc-14843) | 0.6270 | 0.088 | 3 |
Fe5(OF2)4 (mp-773760) | 0.6528 | 0.200 | 3 |
LiFeF4 (mp-777008) | 0.6769 | 0.004 | 3 |
LiVF4 (mp-776621) | 0.6727 | 0.043 | 3 |
Ba2Ca7I18 (mp-766303) | 0.5366 | 0.072 | 3 |
LiVOF3 (mp-764199) | 0.6429 | 0.081 | 4 |
LiFe2OF5 (mp-777198) | 0.7134 | 0.085 | 4 |
GaTeO3F (mp-558984) | 0.6834 | 0.000 | 4 |
FeTeO3F (mp-566335) | 0.6466 | 0.000 | 4 |
LiSbWO6 (mp-19694) | 0.7230 | 0.037 | 4 |
W9C4 (mp-684989) | 0.5573 | 0.083 | 2 |
Fe8N3 (mp-673174) | 0.6577 | 0.017 | 2 |
Fe12N5 (mp-27908) | 0.5560 | 0.025 | 2 |
SbO2 (mp-560098) | 0.6784 | 0.001 | 2 |
SbO2 (mvc-6570) | 0.5550 | 0.137 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Fe_pv N |
Final Energy/Atom-8.4590 eV |
Corrected Energy-592.1272 eV
-592.1272 eV = -592.1272 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)