Final Magnetic Moment1.375 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.070 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.231 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToScS + Sc2S3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 135.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 271.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 226.4 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 317.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 135.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 317.0 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 317.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 271.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 226.4 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 317.0 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 317.0 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 271.7 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 271.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 226.4 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 135.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 181.1 |
BN (mp-984) | <1 0 1> | <0 0 1> | 181.1 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 135.9 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 317.0 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 181.1 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 181.1 |
C (mp-66) | <1 0 0> | <0 0 1> | 317.0 |
C (mp-66) | <1 1 0> | <0 0 1> | 317.0 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 271.7 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 135.9 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 226.4 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 271.7 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 90.6 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 226.4 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 317.0 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 317.0 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 271.7 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 317.0 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 226.4 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 317.0 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 317.0 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 226.4 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 226.4 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 317.0 |
C (mp-48) | <0 0 1> | <0 0 1> | 317.0 |
C (mp-48) | <1 0 1> | <0 0 1> | 181.1 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 271.7 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 271.7 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 226.4 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 317.0 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 317.0 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 317.0 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 317.0 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 226.4 |
TiO2 (mp-390) | <1 0 0> | <0 0 1> | 181.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca17(Y7S19)2 (mp-686346) | 0.4834 | 0.246 | 3 |
Sn(BiTe2)2 (mp-677596) | 0.5292 | 0.030 | 3 |
Ag15Bi7I40 (mp-685512) | 0.5345 | 0.152 | 3 |
InBiS3 (mp-1078776) | 0.5870 | 0.003 | 3 |
Ag5(Sn3S8)2 (mp-530464) | 0.5754 | 0.017 | 3 |
LiCr(CoO3)2 (mp-779929) | 0.5751 | 0.055 | 4 |
LiFe(CoO3)2 (mp-763429) | 0.5661 | 0.060 | 4 |
LiMnCr2O6 (mp-850948) | 0.5786 | 0.097 | 4 |
LiCr2CoO6 (mp-763359) | 0.5685 | 0.096 | 4 |
LiCo2CuO6 (mp-763314) | 0.5983 | 0.112 | 4 |
Zr23S32 (mp-673649) | 0.6691 | 0.026 | 2 |
Tm23Se32 (mp-684691) | 0.6643 | 0.005 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sc_sv S |
Final Energy/Atom-6.7111 eV |
Corrected Energy-504.3530 eV
-504.3530 eV = -476.4877 eV (uncorrected energy) - 27.8653 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)