Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.504 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.448 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.47 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAlN + Sr2Si5N8 + Er2O3 |
Band Gap0.176 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 233.5 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 72.2 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 233.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 233.5 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 166.8 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 216.6 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 133.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 300.2 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 266.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 300.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 288.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 166.8 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 266.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 133.4 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 256.1 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 288.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 256.1 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 192.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 64.0 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 233.5 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 166.8 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 192.0 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 192.0 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 221.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 233.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 233.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 233.5 |
BN (mp-984) | <1 0 0> | <1 0 1> | 288.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 233.5 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 100.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 33.4 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 64.0 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 110.9 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 233.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 192.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 100.1 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 300.2 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 233.5 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 110.9 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 192.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 233.5 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 66.7 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 320.1 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 192.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 320.1 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 133.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 33.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 256.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 133.4 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 233.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MgSiO3 (mp-642216) | 0.7448 | 0.144 | 3 |
Na3Fe5O9 (mp-559275) | 0.6890 | 0.008 | 3 |
Li2Ge4O9 (mp-1020012) | 0.7445 | 0.031 | 3 |
Na3Fe5O9 (mp-654001) | 0.6915 | 0.008 | 3 |
Li4Mn3OF8 (mp-764981) | 0.7066 | 0.079 | 4 |
Li4Cr2Si4O13 (mp-762874) | 0.6938 | 0.040 | 4 |
Li6Co11(OF12)2 (mp-764192) | 0.6900 | 0.069 | 4 |
NaLiGe4O9 (mp-6663) | 0.6302 | 0.010 | 4 |
ZnCu2(NiO4)2 (mvc-10477) | 0.6752 | 0.287 | 4 |
Li4VP2(O4F)2 (mp-782668) | 0.6935 | 0.026 | 5 |
Ba2Ho2Al3Si5N11O3 (mp-684935) | 0.2002 | 0.552 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv Er_3 Al Si N O |
Final Energy/Atom-7.3157 eV |
Corrected Energy-192.3149 eV
-192.3149 eV = -190.2081 eV (uncorrected energy) - 2.1069 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)