Final Magnetic Moment18.915 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-0.675 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.032 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.67 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToV5Se8 + VSe2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CdS (mp-672) | <1 1 0> | <0 0 1> | 255.0 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 105.0 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 170.0 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 255.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 255.0 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 255.0 |
C (mp-66) | <1 0 0> | <0 0 1> | 255.0 |
C (mp-66) | <1 1 0> | <0 0 1> | 255.0 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 255.0 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 255.0 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 210.0 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 255.0 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 105.0 |
MoSe2 (mp-1634) | <1 0 1> | <1 0 0> | 105.0 |
WSe2 (mp-1821) | <1 0 1> | <1 0 0> | 105.0 |
WSe2 (mp-1821) | <1 0 0> | <0 0 1> | 255.0 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 255.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3(VSe2)5 (mp-675310) | 0.7009 | 0.000 | 3 |
LiFeF3 (mp-764373) | 0.6785 | 0.092 | 3 |
Pr3RuI3 (mp-28746) | 0.6914 | 0.000 | 3 |
Pr3OsI3 (mp-570779) | 0.6790 | 0.000 | 3 |
Mg(BiO2)2 (mvc-7302) | 0.6597 | 0.047 | 3 |
Li2Mn2SbO6 (mp-775235) | 0.7325 | 0.090 | 4 |
Li2Co2SiO6 (mp-763534) | 0.6452 | 0.132 | 4 |
Li4Co5NiO12 (mp-772680) | 0.7395 | 0.077 | 4 |
Li2Co(NiO3)2 (mp-761662) | 0.7147 | 0.073 | 4 |
Li2TiMn2O6 (mp-776053) | 0.7275 | 0.072 | 4 |
Tl4O3 (mp-27684) | 0.6885 | 0.000 | 2 |
NaLiV(OF)2 (mp-764851) | 0.7221 | 0.078 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: V_pv Se |
Final Energy/Atom-6.2100 eV |
Corrected Energy-391.2329 eV
-391.2329 eV = -391.2329 eV (uncorrected energy)
|