Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.345 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.108 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.31 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSrAl2O4 + Sr3Al2O6 |
Band Gap1.167 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [146] |
HallR 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba5Sc6O14 (mp-770836) | 0.6041 | 0.060 | 3 |
Na2Ti2O5 (mp-773663) | 0.6300 | 0.055 | 3 |
Sr3Ga4O9 (mp-30158) | 0.6410 | 0.000 | 3 |
Ba3Ga4O9 (mp-771132) | 0.5679 | 0.000 | 3 |
Ca5Al6O14 (mp-17694) | 0.6308 | 0.003 | 3 |
LiBiP2O7 (mp-760629) | 0.7238 | 0.065 | 4 |
Nd4Ga2S5O4 (mp-558333) | 0.7263 | 0.000 | 4 |
Li3Fe(PO4)2 (mp-761514) | 0.6218 | 0.170 | 4 |
LiCaPO4 (mp-16804) | 0.6526 | 0.003 | 4 |
CaSn2(PO4)2 (mvc-9564) | 0.7213 | 0.060 | 4 |
K2LiVPO6 (mp-764301) | 0.6923 | 0.080 | 5 |
KNaZnP2O7 (mp-554157) | 0.7108 | 0.000 | 5 |
KHoCoSi2O7 (mp-735519) | 0.7362 | 0.064 | 5 |
KNaLi2(SO4)2 (mp-14484) | 0.7160 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv Al O |
Final Energy/Atom-7.0478 eV |
Corrected Energy-327.6604 eV
-327.6604 eV = -310.1031 eV (uncorrected energy) - 17.5572 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)