Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.502 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.016 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.45 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTlInSe2 + InSe |
Band Gap0.441 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC222 [21] |
HallC 2 2 |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
Ag (mp-124) | <1 1 0> | <0 0 1> | 243.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 243.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 243.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 243.7 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 243.7 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 243.7 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 243.7 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 243.7 |
Au (mp-81) | <1 1 0> | <0 0 1> | 243.7 |
Au (mp-81) | <1 1 1> | <0 0 1> | 243.7 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 243.7 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 243.7 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 243.7 |
ZnO (mp-2133) | <1 1 0> | <0 0 1> | 243.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tl3In7Se10 (mp-675519) | 0.0511 | 0.034 | 3 |
RbInTe2 (mp-22255) | 0.0670 | 0.000 | 3 |
TlInSe2 (mp-22232) | 0.0464 | 0.000 | 3 |
KInTe2 (mp-19851) | 0.0970 | 0.000 | 3 |
NaAlSe2 (mp-10166) | 0.0812 | 0.015 | 3 |
MnTl2SnTe4 (mp-569859) | 0.2472 | 0.000 | 4 |
Tl2CdSnTe4 (mp-570076) | 0.2841 | 0.009 | 4 |
Rb2SnHgTe4 (mp-1080691) | 0.2649 | 0.000 | 4 |
MnTl2GeTe4 (mp-638590) | 0.2958 | 0.000 | 4 |
Tl2SnHgTe4 (mp-570051) | 0.3151 | 0.012 | 4 |
TlSe (mp-1836) | 0.1816 | 0.000 | 2 |
TlS (mp-322) | 0.2360 | 0.052 | 2 |
InTe (mp-20320) | 0.2792 | 0.011 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tl_d In_d Se |
Final Energy/Atom-3.5482 eV |
Corrected Energy-283.8574 eV
-283.8574 eV = -283.8574 eV (uncorrected energy)
|