Final Magnetic Moment0.827 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.841 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.018 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.26 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBa8Nb7S24 + Nb3S5 + BaS |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 -1> | 237.4 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 161.3 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 1> | 215.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 318.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 318.4 |
LiF (mp-1138) | <1 1 0> | <1 1 -1> | 142.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 238.8 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 242.0 |
Ag (mp-124) | <1 0 0> | <1 -1 0> | 121.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 238.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 238.8 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 238.8 |
BN (mp-984) | <1 1 0> | <0 1 0> | 242.0 |
GaSe (mp-1943) | <1 0 0> | <1 1 0> | 213.6 |
TeO2 (mp-2125) | <1 0 0> | <1 1 -1> | 142.0 |
TeO2 (mp-2125) | <1 0 1> | <0 1 -1> | 237.4 |
MgO (mp-1265) | <1 0 0> | <1 -1 -1> | 145.0 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 318.4 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 238.8 |
C (mp-66) | <1 1 0> | <0 0 1> | 238.8 |
GdScO3 (mp-5690) | <1 1 1> | <0 1 1> | 215.3 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 243.2 |
PbS (mp-21276) | <1 0 0> | <1 -1 -1> | 145.0 |
InP (mp-20351) | <1 0 0> | <1 -1 -1> | 145.0 |
TbScO3 (mp-31119) | <1 1 1> | <0 1 1> | 215.3 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 -1> | 118.7 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 238.8 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 1> | 215.3 |
NdGaO3 (mp-3196) | <1 1 1> | <0 1 1> | 215.3 |
SiC (mp-11714) | <1 0 0> | <1 0 1> | 216.5 |
YAlO3 (mp-3792) | <1 1 1> | <0 0 1> | 238.8 |
Ga2O3 (mp-886) | <1 0 0> | <1 -1 -1> | 145.0 |
Au (mp-81) | <1 0 0> | <1 -1 0> | 121.5 |
Au (mp-81) | <1 1 1> | <0 0 1> | 238.8 |
SrTiO3 (mp-4651) | <1 1 1> | <0 1 1> | 215.3 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 238.8 |
C (mp-48) | <0 0 1> | <0 1 1> | 215.3 |
C (mp-48) | <1 1 0> | <0 0 1> | 238.8 |
Al2O3 (mp-1143) | <1 0 1> | <0 0 1> | 318.4 |
CdWO4 (mp-19387) | <0 0 1> | <1 1 1> | 123.7 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 243.2 |
MgF2 (mp-1249) | <1 1 1> | <0 0 1> | 238.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Nb_pv S |
Final Energy/Atom-6.1645 eV |
Corrected Energy-183.8846 eV
-183.8846 eV = -172.6058 eV (uncorrected energy) - 11.2788 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)