Final Magnetic Moment0.553 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.373 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.041 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.29 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAgI + BiI3 + I |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 278.1 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 278.1 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 278.1 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 278.1 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 278.1 |
BN (mp-984) | <1 1 0> | <0 0 1> | 69.5 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 208.5 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 278.1 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 278.1 |
MoSe2 (mp-1634) | <1 1 1> | <0 0 1> | 278.1 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 278.1 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 278.1 |
C (mp-48) | <1 0 0> | <0 0 1> | 208.5 |
C (mp-48) | <1 1 0> | <0 0 1> | 69.5 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 278.1 |
GaSb (mp-1156) | <1 1 0> | <0 0 1> | 278.1 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 208.5 |
C (mp-48) | <0 0 1> | <0 0 1> | 278.1 |
ZnO (mp-2133) | <1 1 0> | <0 0 1> | 278.1 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 278.1 |
ZnTe (mp-2176) | <1 1 0> | <0 0 1> | 278.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ag15(BiI4)16 (mp-686149) | 0.0455 | 0.042 | 3 |
Ag13Bi15I64 (mp-685283) | 0.7354 | 0.108 | 3 |
LiVF4 (mp-766911) | 0.7031 | 0.089 | 3 |
LiVOF3 (mp-764237) | 0.7444 | 0.259 | 4 |
Mn15O32 (mp-777108) | 0.6160 | 0.097 | 2 |
Fe24N11 (mp-684887) | 0.7128 | 0.174 | 2 |
Mn15O32 (mp-868759) | 0.6276 | 0.101 | 2 |
Zr63S128 (mp-1024087) | 0.5044 | 0.029 | 2 |
Sc12I25 (mp-685088) | 0.5937 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ag Bi I |
Final Energy/Atom-2.5007 eV |
Corrected Energy-207.5621 eV
-207.5621 eV = -207.5621 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)