Final Magnetic Moment0.033 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.032 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.119 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.55 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSrLaGa3O7 + Mg(GaO2)2 + La4Ga2O9 + MgO + Ga |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 26.9 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 214.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 107.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 295.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 214.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 214.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 161.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 322.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 241.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 26.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 295.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 268.6 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 214.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 188.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 161.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 214.9 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 53.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 322.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 53.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 322.3 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 214.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 161.2 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 322.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 241.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 80.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 161.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 26.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 107.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 268.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 295.5 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 349.2 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 295.5 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 188.0 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 214.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 349.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 295.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 349.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 349.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 322.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 241.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 295.5 |
BN (mp-984) | <1 0 0> | <0 0 1> | 349.2 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 322.3 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 134.3 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 322.3 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 161.2 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 295.5 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 107.4 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 322.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 107.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca4Mn4O11 (mp-698549) | 0.6609 | 0.061 | 3 |
Ba5Bi5O13 (mp-674987) | 0.5513 | 0.056 | 3 |
La18Ni12O41 (mp-868889) | 0.6653 | 0.057 | 3 |
La7Mn8O23 (mp-763886) | 0.5052 | 0.236 | 3 |
La16Mg2Ga14O47 (mp-695096) | 0.5948 | 0.066 | 4 |
Ba2Tb2Mn4O11 (mp-868127) | 0.7202 | 0.001 | 4 |
Sr2La14Mg4(Ga4O15)3 (mp-686724) | 0.6272 | 0.103 | 5 |
Sr2La14Mg4(Ga4O15)3 (mp-686367) | 0.4606 | 0.119 | 5 |
SrLa11Mg3Ga9O34 (mp-677725) | 0.5111 | 0.110 | 5 |
SrLa9MgGa9O29 (mp-677649) | 0.4497 | 0.084 | 5 |
SrLa11Mg3Ga9O34 (mp-677081) | 0.4496 | 0.111 | 5 |
SrLa9Mg2Ga6(FeO14)2 (mp-705586) | 0.4303 | 0.114 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv La Mg_pv Ga_d O |
Final Energy/Atom-7.0468 eV |
Corrected Energy-574.2040 eV
-574.2040 eV = -542.6009 eV (uncorrected energy) - 31.6030 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)