Final Magnetic Moment0.011 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-0.383 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.640 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.54 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAgCl + H2O + H4NCl + Ag + N2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 282.3 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 248.5 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 282.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 142.5 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 142.5 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 297.1 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 222.8 |
CeO2 (mp-20194) | <1 1 0> | <0 1 -1> | 303.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 212.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 297.1 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 288.5 |
SiO2 (mp-6930) | <0 0 1> | <1 0 -1> | 288.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 288.5 |
Ag (mp-124) | <1 0 0> | <0 1 -1> | 227.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 222.8 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 297.1 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 248.5 |
GaSe (mp-1943) | <1 0 1> | <1 -1 1> | 207.6 |
Te2W (mp-22693) | <1 0 0> | <0 1 0> | 297.1 |
YVO4 (mp-19133) | <1 1 1> | <0 1 1> | 248.5 |
Te2Mo (mp-602) | <0 0 1> | <1 -1 1> | 207.6 |
BN (mp-984) | <1 0 0> | <0 1 0> | 297.1 |
BN (mp-984) | <1 0 1> | <1 0 0> | 141.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 142.5 |
Al (mp-134) | <1 0 0> | <1 1 0> | 212.4 |
Al (mp-134) | <1 1 0> | <0 1 0> | 297.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 -1> | 227.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 1> | 208.5 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 -1> | 288.5 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 0> | 282.3 |
SiC (mp-7631) | <1 1 0> | <0 1 1> | 248.5 |
SiC (mp-7631) | <1 1 1> | <0 1 1> | 248.5 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 282.3 |
MgO (mp-1265) | <1 0 0> | <1 0 -1> | 288.5 |
C (mp-66) | <1 0 0> | <0 1 0> | 297.1 |
C (mp-66) | <1 1 0> | <1 0 -1> | 288.5 |
C (mp-66) | <1 1 1> | <1 0 -1> | 288.5 |
TiO2 (mp-2657) | <1 0 0> | <1 -1 1> | 207.6 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 -1> | 227.6 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 213.8 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 282.3 |
Mg (mp-153) | <1 1 0> | <1 -1 0> | 295.7 |
Mg (mp-153) | <0 0 1> | <0 1 -1> | 227.6 |
GaP (mp-2490) | <1 1 0> | <0 1 -1> | 303.5 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 285.1 |
InP (mp-20351) | <1 1 0> | <0 1 1> | 248.5 |
TbScO3 (mp-31119) | <0 0 1> | <0 1 -1> | 227.6 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 282.3 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 -1> | 303.5 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 -1> | 288.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaH9O5 (mp-626165) | 0.6767 | 0.052 | 3 |
H8N2O (mp-625815) | 0.6714 | 0.239 | 3 |
H9BrO4 (mp-625596) | 0.6229 | 0.022 | 3 |
NaH9O5 (mp-625501) | 0.7037 | 0.028 | 3 |
NaH9O5 (mp-625455) | 0.5812 | 0.050 | 3 |
NaH5S2O9 (mp-733973) | 0.6305 | 0.555 | 4 |
ZnH12(IN2)2 (mp-707471) | 0.7033 | 0.618 | 4 |
MgH12SO9 (mp-697114) | 0.5453 | 0.312 | 4 |
CaH8(BrO6)2 (mp-745067) | 0.5392 | 0.096 | 4 |
AlH18(BrO6)3 (mp-695979) | 0.5117 | 0.304 | 4 |
KFeH5(SO5)2 (mp-694884) | 0.7086 | 0.533 | 5 |
LaH12S2NO12 (mp-707989) | 0.7402 | 0.429 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ag H N Cl O |
Final Energy/Atom-4.5288 eV |
Corrected Energy-186.6487 eV
Uncorrected energy = -181.1527 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Corrected energy = -186.6487 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)