Final Magnetic Moment1.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.848 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.315 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.85 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSrCuO2 + LaCuO2 + Sr(BiO2)2 |
Band Gap0.623 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 99.9 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 272.5 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 1> | 299.6 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 99.9 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 286.4 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 173.2 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 141.6 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 199.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 257.6 |
Te2Mo (mp-602) | <1 0 1> | <1 -1 -1> | 165.4 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 272.5 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 1> | 286.4 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 257.6 |
MoS2 (mp-1434) | <1 0 0> | <0 1 1> | 199.8 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 1> | 286.4 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 199.8 |
TePb (mp-19717) | <1 1 1> | <0 1 1> | 299.6 |
Te2Mo (mp-602) | <0 0 1> | <1 -1 -1> | 165.4 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 257.6 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 257.6 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 1> | 299.6 |
CdTe (mp-406) | <1 1 1> | <0 1 1> | 299.6 |
SiC (mp-7631) | <0 0 1> | <0 1 1> | 99.9 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 257.6 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 257.6 |
TiO2 (mp-2657) | <0 0 1> | <0 1 1> | 299.6 |
TiO2 (mp-2657) | <1 1 1> | <1 1 1> | 286.4 |
InSb (mp-20012) | <1 1 1> | <0 1 1> | 299.6 |
PbSe (mp-2201) | <1 1 0> | <0 1 0> | 259.9 |
C (mp-66) | <1 0 0> | <1 1 1> | 190.9 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 272.5 |
BaTiO3 (mp-5986) | <1 1 0> | <1 1 -1> | 166.6 |
Mg (mp-153) | <1 0 0> | <0 1 1> | 99.9 |
Mg (mp-153) | <1 1 0> | <1 1 1> | 286.4 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 1 1> | 299.6 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 257.6 |
NdGaO3 (mp-3196) | <1 1 1> | <0 1 1> | 199.8 |
SiC (mp-11714) | <0 0 1> | <0 1 1> | 99.9 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 257.6 |
SiC (mp-11714) | <1 1 1> | <1 1 -1> | 166.6 |
Au (mp-81) | <1 1 0> | <1 0 0> | 272.5 |
MoSe2 (mp-1634) | <0 0 1> | <1 -1 0> | 143.0 |
CdSe (mp-2691) | <1 1 0> | <0 1 0> | 259.9 |
ZrO2 (mp-2858) | <0 1 0> | <1 1 1> | 286.4 |
ZrO2 (mp-2858) | <1 0 0> | <1 1 1> | 286.4 |
ZrO2 (mp-2858) | <1 0 1> | <0 1 1> | 299.6 |
C (mp-48) | <1 1 0> | <1 0 0> | 272.5 |
C (mp-48) | <1 1 1> | <1 0 0> | 272.5 |
WSe2 (mp-1821) | <0 0 1> | <1 -1 0> | 143.0 |
YAlO3 (mp-3792) | <0 1 1> | <1 1 1> | 95.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv La Cu_pv Bi O |
Final Energy/Atom-5.7535 eV |
Corrected Energy-264.3455 eV
-264.3455 eV = -253.1562 eV (uncorrected energy) - 11.1893 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)