Final Magnetic Moment2.138 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.381 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.123 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.41 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiFe(PO3)4 + P2O5 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 1 0> | 276.1 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 276.1 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 276.1 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 170.4 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 142.0 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 276.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 -1> | 193.7 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 170.4 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 184.1 |
BN (mp-984) | <1 0 0> | <0 1 1> | 154.7 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 142.0 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 124.3 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 124.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 276.1 |
Mg (mp-153) | <1 0 1> | <1 0 -1> | 170.4 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 142.0 |
LiTaO3 (mp-3666) | <1 1 0> | <0 0 1> | 124.3 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 184.1 |
PbSe (mp-2201) | <1 1 0> | <0 1 0> | 276.1 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 248.6 |
WSe2 (mp-1821) | <1 0 0> | <0 0 1> | 248.6 |
SiC (mp-11714) | <1 1 0> | <0 1 0> | 276.1 |
YAlO3 (mp-3792) | <0 1 0> | <0 1 0> | 276.1 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 248.6 |
SiC (mp-8062) | <1 1 0> | <0 1 0> | 276.1 |
CdSe (mp-2691) | <1 1 0> | <0 1 0> | 276.1 |
C (mp-48) | <0 0 1> | <0 1 0> | 184.1 |
NaCl (mp-22862) | <1 0 0> | <1 1 -1> | 193.7 |
TiO2 (mp-390) | <1 0 0> | <0 1 0> | 184.1 |
ZrO2 (mp-2858) | <0 0 1> | <0 1 0> | 276.1 |
ZrO2 (mp-2858) | <0 1 0> | <0 1 0> | 276.1 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 0> | 142.0 |
ZnO (mp-2133) | <1 0 0> | <0 1 0> | 276.1 |
YAlO3 (mp-3792) | <0 0 1> | <0 1 0> | 276.1 |
YAlO3 (mp-3792) | <1 0 0> | <0 1 0> | 276.1 |
YAlO3 (mp-3792) | <1 1 0> | <0 1 0> | 276.1 |
GaSb (mp-1156) | <1 1 0> | <0 1 0> | 276.1 |
LiAlO2 (mp-3427) | <0 0 1> | <0 1 0> | 276.1 |
Fe2O3 (mp-24972) | <1 0 0> | <1 0 0> | 142.0 |
Fe2O3 (mp-24972) | <1 1 0> | <0 0 1> | 124.3 |
ZnTe (mp-2176) | <1 1 0> | <0 1 0> | 276.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NiP4O11 (mp-764190) | 0.4745 | 0.009 | 3 |
Fe(PO3)4 (mp-31874) | 0.4847 | 0.095 | 3 |
CoP4O11 (mp-763297) | 0.4846 | 0.126 | 3 |
CdP4O11 (mp-772228) | 0.4656 | 0.000 | 3 |
Co(PO3)4 (mp-31550) | 0.4646 | 0.062 | 3 |
LiP5WO15 (mp-773952) | 0.3638 | 0.031 | 4 |
LiCo(PO3)5 (mp-705372) | 0.0884 | 0.057 | 4 |
LiCr(PO3)5 (mp-705315) | 0.1268 | 0.086 | 4 |
LiV(PO3)5 (mp-705281) | 0.3419 | 0.055 | 4 |
LiTi(PO3)5 (mp-684119) | 0.3375 | 0.028 | 4 |
MgCr3Se2(SO6)4 (mp-769544) | 0.7050 | 0.126 | 5 |
MnVP2(O4F)2 (mp-777435) | 0.7190 | 0.002 | 5 |
MgCr3Se3(SO8)3 (mp-773999) | 0.6720 | 0.180 | 5 |
Cs3Mg3In(PO3)12 (mp-720658) | 0.6332 | 0.006 | 5 |
K5Li3Ti8(AsO5)8 (mp-766047) | 0.7090 | 0.007 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P O |
Final Energy/Atom-6.8536 eV |
Corrected Energy-653.3594 eV
Uncorrected energy = -603.1154 eV
Composition-based energy adjustment (-0.687 eV/atom x 60.0 atoms) = -41.2200 eV
Composition-based energy adjustment (-2.256 eV/atom x 4.0 atoms) = -9.0240 eV
Corrected energy = -653.3594 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)