Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.315 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.028 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.71 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2CN2 + CsN3 + Cs2CN2 + C + CoN |
Band Gap4.302 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
InAs (mp-20305) | <1 1 1> | <1 1 1> | 194.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 194.9 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 112.5 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 194.9 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 159.1 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 1 0> | 159.1 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 159.1 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 159.1 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 225.1 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 225.1 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 159.1 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 225.1 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 1> | 194.9 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 225.1 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 225.1 |
Au (mp-81) | <1 0 0> | <1 0 0> | 225.1 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 112.5 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <1 1 1> | 194.9 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 159.1 |
CdSe (mp-2691) | <1 1 1> | <1 1 1> | 194.9 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 112.5 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 112.5 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <1 1 1> | 194.9 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 112.5 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 225.1 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 0> | 112.5 |
YAlO3 (mp-3792) | <0 1 0> | <1 1 0> | 159.1 |
YAlO3 (mp-3792) | <1 0 0> | <1 1 0> | 159.1 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 112.5 |
TiO2 (mp-390) | <1 0 1> | <1 1 0> | 159.1 |
C (mp-48) | <0 0 1> | <1 1 1> | 194.9 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <1 0 0> | 112.5 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <1 1 0> | 159.1 |
ZnTe (mp-2176) | <1 1 0> | <1 1 0> | 159.1 |
GaTe (mp-542812) | <1 0 0> | <1 0 0> | 225.1 |
ZnTe (mp-2176) | <1 1 1> | <1 1 1> | 194.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CsMn(CN)3 (mp-863692) | 0.5097 | 0.024 | 4 |
FeNi2(CN)6 (mp-21498) | 0.7275 | 0.579 | 4 |
FeCu2(CN)6 (mp-22413) | 0.6576 | 0.573 | 4 |
Cs2MgFe(CN)6 (mp-7331) | 0.1345 | 0.000 | 5 |
Cs2LiMn(CN)6 (mp-6854) | 0.1688 | 0.125 | 5 |
Rb2FeCu(CN)6 (mp-20140) | 0.2415 | 0.188 | 5 |
Cs2ZnFe(CN)6 (mp-570545) | 0.1905 | 0.009 | 5 |
Cs2LiFe(CN)6 (mp-21013) | 0.0782 | 0.101 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv Li_sv Co C N |
Final Energy/Atom-7.4331 eV |
Corrected Energy-121.0961 eV
Uncorrected energy = -118.9301 eV
Composition-based energy adjustment (-0.361 eV/atom x 6.0 atoms) = -2.1660 eV
Corrected energy = -121.0961 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)