material

VMoO5

ID:

mp-690110

DOI:

10.17188/1284466


Material Details

Final Magnetic Moment
1.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-2.161 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.060 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.22 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
MoO3 + VO2
Band Gap
1.006 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cm [8]
Hall
C 2y
Point Group
m
Crystal System
monoclinic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiC (mp-8062) <1 0 0> <0 1 0> 0.005 327.0
Ag (mp-124) <1 1 0> <1 0 -1> 0.017 218.7
BN (mp-984) <1 0 0> <1 1 0> 0.021 212.0
GaSe (mp-1943) <1 0 0> <1 0 -1> 0.023 136.7
GaSe (mp-1943) <1 0 1> <1 0 -1> 0.027 136.7
YVO4 (mp-19133) <1 0 0> <1 0 -1> 0.032 136.7
NdGaO3 (mp-3196) <0 1 0> <0 0 1> 0.034 256.5
LiTaO3 (mp-3666) <1 1 1> <0 0 1> 0.035 256.5
WS2 (mp-224) <1 0 1> <1 1 -1> 0.046 324.7
Au (mp-81) <1 1 0> <1 0 -1> 0.046 218.7
MgO (mp-1265) <1 0 0> <0 1 1> 0.054 237.5
GaP (mp-2490) <1 1 0> <0 0 1> 0.057 256.5
CdS (mp-672) <1 0 1> <1 0 -1> 0.062 164.0
CdWO4 (mp-19387) <0 0 1> <1 1 0> 0.065 212.0
LiAlO2 (mp-3427) <1 1 0> <1 0 1> 0.065 282.4
WSe2 (mp-1821) <1 1 1> <1 1 0> 0.066 264.9
GaN (mp-804) <1 1 0> <1 0 0> 0.071 175.1
Si (mp-149) <1 1 0> <0 0 1> 0.072 256.5
DyScO3 (mp-31120) <1 0 1> <0 0 1> 0.073 109.9
TiO2 (mp-2657) <1 1 1> <1 0 0> 0.075 175.1
ZnO (mp-2133) <0 0 1> <1 0 0> 0.075 75.0
TiO2 (mp-390) <0 0 1> <0 0 1> 0.076 73.3
CeO2 (mp-20194) <1 1 0> <0 0 1> 0.077 256.5
C (mp-66) <1 0 0> <1 0 -1> 0.078 218.7
AlN (mp-661) <1 1 1> <0 1 0> 0.082 140.1
Te2W (mp-22693) <1 0 0> <0 0 1> 0.083 293.1
CaF2 (mp-2741) <1 1 0> <0 0 1> 0.090 256.5
ZrO2 (mp-2858) <0 1 1> <1 1 0> 0.093 159.0
Ge (mp-32) <1 0 0> <1 0 -1> 0.097 300.7
CaCO3 (mp-3953) <1 0 0> <1 0 0> 0.098 175.1
GaSe (mp-1943) <0 0 1> <1 0 0> 0.102 25.0
BN (mp-984) <1 0 1> <1 1 0> 0.104 264.9
Ni (mp-23) <1 1 1> <1 0 0> 0.105 150.1
LiGaO2 (mp-5854) <0 0 1> <1 0 0> 0.106 225.1
ZrO2 (mp-2858) <1 1 0> <0 1 1> 0.107 118.7
ZnO (mp-2133) <1 0 0> <1 0 0> 0.108 175.1
Ga2O3 (mp-886) <1 1 0> <0 1 1> 0.111 296.8
LiNbO3 (mp-3731) <1 1 1> <0 0 1> 0.113 256.5
TiO2 (mp-390) <1 0 0> <0 0 1> 0.131 36.6
GaAs (mp-2534) <1 0 0> <1 0 -1> 0.131 300.7
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.136 100.1
YVO4 (mp-19133) <1 0 1> <1 0 -1> 0.141 136.7
TbScO3 (mp-31119) <1 0 1> <0 0 1> 0.142 109.9
Bi2Te3 (mp-34202) <0 0 1> <1 0 -1> 0.145 218.7
CdWO4 (mp-19387) <1 0 0> <1 0 -1> 0.149 191.4
SiC (mp-7631) <1 0 1> <0 1 1> 0.154 237.5
BaTiO3 (mp-5986) <1 1 0> <1 1 -1> 0.155 216.5
C (mp-48) <1 0 1> <1 1 0> 0.157 159.0
LiF (mp-1138) <1 1 1> <1 0 0> 0.158 175.1
ZnO (mp-2133) <1 0 1> <1 1 -1> 0.159 216.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
72 62 50 0 -15 0
62 298 47 0 -17 0
50 47 208 0 -17 0
0 0 0 39 0 -6
-15 -17 -17 0 37 0
0 0 0 -6 0 50
Compliance Tensor Sij (10-12Pa-1)
20.5 -3.4 -3.7 0 4.8 0
-3.4 4.1 -0.1 0 0.5 0
-3.7 -0.1 5.8 0 1.2 0
0 0 0 26.3 0 3.1
4.8 0.5 1.2 0 29.7 0
0 0 0 3.1 0 20.3
Shear Modulus GV
53 GPa
Bulk Modulus KV
100 GPa
Shear Modulus GR
40 GPa
Bulk Modulus KR
63 GPa
Shear Modulus GVRH
46 GPa
Bulk Modulus KVRH
81 GPa
Elastic Anisotropy
2.30
Poisson's Ratio
0.26

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
-1.19560 -0.39516 -0.27700 0.00032 0.00161 -0.31831
-0.31831 -0.42549 -0.26035 0.00042 0.00032 -0.39516
0.00161 0.00042 0.00092 -0.26035 -0.27700 0.00032
Piezoelectric Modulus ‖eijmax
1.45295 C/m2
Crystallographic Direction vmax
-0.90667
0.42181
0.00501

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
5.89 0.97 -0.01
0.97 5.92 0.00
-0.01 0.00 6.53
Dielectric Tensor εij (total)
19.60 9.98 -0.02
9.98 23.99 -0.01
-0.02 -0.01 66.62
Polycrystalline dielectric constant εpoly
(electronic contribution)
2.03
Polycrystalline dielectric constant εpoly
(total)
2.03
Refractive Index n
1.43
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
VH2SeO5 (mp-743869) 0.6200 0.025 4
Rb2Nb3Cl7O5 (mp-558393) 0.6127 0.000 4
K2Nb3Cl7O5 (mp-559790) 0.6305 0.000 4
TbCu(WO4)2 (mp-565849) 0.6229 0.051 4
NaH3(SeO3)2 (mp-696842) 0.5773 0.008 4
V6O13 (mp-714921) 0.7085 0.027 2
TiO2 (mp-554278) 0.7133 0.000 2
V2O5 (mp-25646) 0.6929 0.029 2
V6O13 (mp-715617) 0.6806 0.045 2
ZrO2 (mp-755769) 0.6857 0.053 2
YV3O9 (mvc-13592) 0.6411 0.126 3
GeWO4 (mp-773397) 0.6069 0.175 3
V6CuO15 (mp-763150) 0.6523 0.033 3
Sb(MoO4)2 (mp-510758) 0.6588 0.141 3
LiVF4 (mp-777556) 0.6519 0.074 3
RbMnH4Cl3O2 (mp-25567) 0.6696 0.000 5
ZnH8C2(SN3)2 (mp-696420) 0.7224 0.146 5
KMnH4Cl3O2 (mp-743617) 0.5677 0.000 5
SbRu2C6Cl7O6 (mp-662588) 0.6978 0.048 5
SbIrC2(OF3)2 (mp-557748) 0.7019 0.091 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
V: 3.25 eV
Mo: 4.38 eV
Pseudopotentials
VASP PAW: V_pv Mo_pv O
Final Energy/Atom
-7.2902 eV
Corrected Energy
-59.7560 eV
-59.7560 eV = -51.0316 eV (uncorrected energy) - 5.2130 eV (MP Advanced Correction) - 3.5114 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)