Final Magnetic Moment14.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.694 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.254 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.04 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLa5Mn5O16 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 77.2 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 77.2 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 196.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 237.3 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 148.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 178.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 237.3 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 196.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 29.7 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 130.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 267.0 |
GaAs (mp-2534) | <1 1 1> | <1 0 1> | 231.6 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 323.6 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 326.3 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 326.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 89.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 267.0 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 261.3 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 237.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 237.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 89.0 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 -1> | 179.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 154.3 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 207.7 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 207.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 148.3 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 323.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 267.0 |
ZnSe (mp-1190) | <1 1 1> | <1 0 1> | 231.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 148.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 148.3 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 323.6 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 296.7 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 267.0 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 326.3 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 308.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 148.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 237.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 267.0 |
Te2Mo (mp-602) | <1 1 1> | <0 1 0> | 194.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 148.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 326.3 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 267.0 |
GaSe (mp-1943) | <1 0 1> | <1 -1 -1> | 284.5 |
BN (mp-984) | <1 1 0> | <0 0 1> | 237.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 148.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 59.3 |
BN (mp-984) | <1 0 1> | <0 1 0> | 323.6 |
MoS2 (mp-1434) | <1 1 0> | <0 0 1> | 118.7 |
Al (mp-134) | <1 0 0> | <0 0 1> | 148.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
La3Mn3O10 (mp-761423) | 0.3880 | 0.237 | 3 |
La17Mn17O54 (mp-705870) | 0.3955 | 0.228 | 3 |
La14Mn15O48 (mp-705798) | 0.3689 | 0.222 | 3 |
La5Mn5O16 (mp-705775) | 0.4748 | 0.000 | 3 |
La19Mn19O60 (mp-705671) | 0.4796 | 0.220 | 3 |
LiLa5Ti8O24 (mp-767070) | 0.6785 | 0.039 | 4 |
LaVCrO6 (mvc-10016) | 0.6742 | 0.318 | 4 |
SrTa2Bi2O9 (mp-23089) | 0.5996 | 0.000 | 4 |
La2Ti2CrO9 (mp-767602) | 0.7062 | 0.053 | 4 |
LaCrNiO6 (mvc-10039) | 0.6786 | 0.279 | 4 |
Na2LiLa3Ti6O18 (mp-676447) | 0.6597 | 0.025 | 5 |
CaLa2Ti2Mn2O12 (mvc-14929) | 0.7163 | 0.132 | 5 |
SrLaTa2(NO)3 (mp-694929) | 0.6783 | 0.019 | 5 |
TiNb2Zn(PbO3)4 (mp-684723) | 0.6841 | 0.053 | 5 |
TiNb2Zn(PbO3)4 (mp-684721) | 0.7274 | 0.059 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: La Mn_pv O |
Final Energy/Atom-7.6402 eV |
Corrected Energy-234.9707 eV
-234.9707 eV = -213.9252 eV (uncorrected energy) - 12.6412 eV (MP Anion Correction) - 8.4043 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)