Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-3.048 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.90 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.861 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4mm [107] |
HallI 4 2 |
Point Groupmm2 |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 108.0 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 180.1 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 180.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 36.0 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 50.1 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 61.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 360.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 288.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 108.0 |
BN (mp-984) | <1 0 0> | <1 0 1> | 308.7 |
BN (mp-984) | <1 1 0> | <0 0 1> | 324.1 |
BN (mp-984) | <1 1 1> | <1 0 0> | 250.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 180.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 250.7 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 123.5 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 200.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 144.1 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 1> | 185.2 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 1> | 308.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 180.1 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 0> | 250.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 288.1 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 141.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 324.1 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 250.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 180.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 216.1 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 250.7 |
Al (mp-134) | <1 0 0> | <0 0 1> | 144.1 |
Al (mp-134) | <1 1 0> | <1 0 0> | 200.6 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 324.1 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 150.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 108.0 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 141.8 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 252.1 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 300.8 |
LiGaO2 (mp-5854) | <0 1 1> | <1 1 0> | 212.7 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 216.1 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 180.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 324.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 283.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 324.1 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 283.6 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 200.6 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 288.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 324.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 288.1 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 141.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 144.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 200.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.05189 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | -0.05189 | 0.00000 | 0.00000 |
0.07293 | 0.07293 | 0.52847 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.53844 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
0.00000 |
1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.21 | 0.00 | 0.00 |
0.00 | 2.21 | 0.00 |
0.00 | 0.00 | 2.42 |
Dielectric Tensor εij (total) |
||
---|---|---|
9.21 | 0.00 | 0.00 |
0.00 | 9.21 | 0.00 |
0.00 | 0.00 | 8.13 |
Polycrystalline dielectric constant
εpoly∞
2.28
|
Polycrystalline dielectric constant
εpoly
8.85
|
Refractive Index n1.51 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cs3CeF6 (mp-632715) | 0.3794 | 0.000 | 3 |
Cs3TbF6 (mp-696965) | 0.3845 | 0.000 | 3 |
Ba3WO6 (mp-25172) | 0.3964 | 0.068 | 3 |
Co(N2Cl)3 (mp-1080142) | 0.3739 | 2.627 | 3 |
CsTlF3 (mp-1078203) | 0.4038 | 0.000 | 3 |
Sr2YCoO6 (mp-1080434) | 0.3464 | 0.065 | 4 |
K4BaU3O12 (mp-19965) | 0.3727 | 0.036 | 4 |
K2NaAlF6 (mp-6586) | 0.3690 | 0.000 | 4 |
K9U6BiO24 (mp-558206) | 0.3300 | 0.000 | 4 |
Sr2LaCoO6 (mp-1080670) | 0.3496 | 0.158 | 4 |
K2NaNb(OF2)2 (mp-684816) | 0.3042 | 0.089 | 5 |
Cs2KZrOF5 (mp-40143) | 0.2438 | 0.000 | 5 |
KRb2ZrOF5 (mp-39542) | 0.2114 | 0.020 | 5 |
KZrTl2OF5 (mp-40204) | 0.3442 | 0.058 | 5 |
K2NaTiOF5 (mp-42190) | 0.1630 | 0.000 | 5 |
Ba3LaZnReWO12 (mp-705508) | 0.5792 | 0.057 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: K_sv Na_pv V_pv O F |
Final Energy/Atom-5.2765 eV |
Corrected Energy-220.5955 eV
-220.5955 eV = -211.0583 eV (uncorrected energy) - 6.7280 eV (MP Advanced Correction) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)