material

Na2H6Pt

ID:

mp-690785

DOI:

10.17188/1284576


Tags: Disodium hexadeuterioplatinate(IV)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-0.452 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.10 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
3.615 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MgO (mp-1265) <1 1 0> <1 1 0> 0.000 76.9
MgO (mp-1265) <1 1 1> <1 1 1> 0.000 94.1
C (mp-66) <1 0 0> <1 0 0> 0.000 217.4
C (mp-66) <1 1 0> <1 1 0> 0.000 307.4
LiTaO3 (mp-3666) <0 0 1> <1 1 1> 0.000 94.1
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.000 271.7
LiF (mp-1138) <1 0 0> <1 0 0> 0.001 217.4
KCl (mp-23193) <1 1 0> <1 1 0> 0.001 230.6
KCl (mp-23193) <1 1 1> <1 1 1> 0.001 282.4
LiNbO3 (mp-3731) <0 0 1> <1 1 1> 0.002 94.1
GaP (mp-2490) <1 0 0> <1 0 0> 0.002 271.7
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.002 108.7
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.002 282.4
PbS (mp-21276) <1 1 0> <1 1 0> 0.003 153.7
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.004 54.3
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.006 271.7
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.006 271.7
TePb (mp-19717) <1 0 0> <1 0 0> 0.007 217.4
Mg (mp-153) <1 1 0> <1 1 0> 0.007 230.6
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.007 217.4
Si (mp-149) <1 0 0> <1 0 0> 0.009 271.7
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.010 271.7
CdTe (mp-406) <1 0 0> <1 0 0> 0.011 217.4
InSb (mp-20012) <1 0 0> <1 0 0> 0.014 217.4
GaN (mp-804) <1 1 0> <1 1 0> 0.016 230.6
BaTiO3 (mp-5986) <1 0 0> <1 1 0> 0.017 153.7
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.018 108.7
Mg (mp-153) <0 0 1> <1 1 0> 0.022 307.4
InP (mp-20351) <1 1 1> <1 1 0> 0.022 307.4
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.022 76.9
GaN (mp-804) <1 0 0> <1 0 0> 0.024 271.7
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.024 54.3
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.024 307.4
WS2 (mp-224) <0 0 1> <1 1 0> 0.024 307.4
LiAlO2 (mp-3427) <1 1 0> <1 1 0> 0.025 230.6
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.027 271.7
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.029 271.7
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.031 282.4
Te2Mo (mp-602) <1 0 1> <1 1 1> 0.031 282.4
Ni (mp-23) <1 1 1> <1 1 1> 0.035 282.4
C (mp-66) <1 1 1> <1 1 1> 0.035 282.4
Ni (mp-23) <1 0 0> <1 0 0> 0.035 108.7
Ni (mp-23) <1 1 0> <1 1 0> 0.036 153.7
Ag (mp-124) <1 0 0> <1 0 0> 0.036 271.7
LaF3 (mp-905) <1 0 0> <1 0 0> 0.040 54.3
InP (mp-20351) <1 1 0> <1 1 0> 0.042 153.7
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.046 230.6
ZrO2 (mp-2858) <1 0 -1> <1 1 1> 0.046 282.4
PbS (mp-21276) <1 1 1> <1 1 0> 0.047 307.4
Ge (mp-32) <1 0 0> <1 0 0> 0.049 271.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
43 13 13 0 0 0
13 43 13 0 0 0
13 13 43 0 0 0
0 0 0 16 0 0
0 0 0 0 16 0
0 0 0 0 0 16
Compliance Tensor Sij (10-12Pa-1)
27 -6.3 -6.3 0 0 0
-6.3 27 -6.3 0 0 0
-6.3 -6.3 27 0 0 0
0 0 0 62.2 0 0
0 0 0 0 62.2 0
0 0 0 0 0 62.2
Shear Modulus GV
16 GPa
Bulk Modulus KV
23 GPa
Shear Modulus GR
16 GPa
Bulk Modulus KR
23 GPa
Shear Modulus GVRH
16 GPa
Bulk Modulus KVRH
23 GPa
Elastic Anisotropy
0.01
Poisson's Ratio
0.23

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
3.23 0.00 0.00
0.00 3.23 0.00
0.00 0.00 3.23
Dielectric Tensor εij (total)
7.51 0.00 0.00
0.00 7.51 0.00
0.00 0.00 7.51
Polycrystalline dielectric constant εpoly
(electronic contribution)
3.23
Polycrystalline dielectric constant εpoly
(total)
7.51
Refractive Index n
1.80
Potentially ferroelectric?
True

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
10
U Values
--
Pseudopotentials
VASP PAW: Na_pv H Pt
Final Energy/Atom
-3.5764 eV
Corrected Energy
-32.1876 eV
-32.1876 eV = -32.1876 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 41863