material

FeOF

ID:

mp-691107

DOI:

10.17188/1284609

Warnings: [?]
  1. Large change in a lattice parameter during relaxation.
  2. Large change in volume during relaxation.

Material Details

Final Magnetic Moment
20.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-2.213 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.068 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.34 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Fe2O3 + FeF3
Band Gap
1.692 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P41212 [92]
Hall
P 4abw 2nw
Point Group
422
Crystal System
tetragonal

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KCl (mp-23193) <1 0 0> <0 0 1> 0.000 204.3
Ge3(BiO3)4 (mp-23560) <1 0 0> <0 0 1> 0.001 113.5
KP(HO2)2 (mp-23959) <0 0 1> <0 0 1> 0.001 227.0
MgO (mp-1265) <1 0 0> <0 0 1> 0.002 90.8
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.008 295.2
YAlO3 (mp-3792) <0 1 1> <1 1 0> 0.011 288.6
GaN (mp-804) <0 0 1> <1 1 0> 0.011 206.1
Ga2O3 (mp-886) <1 0 1> <1 0 1> 0.013 184.8
GaAs (mp-2534) <1 0 0> <0 0 1> 0.018 295.2
LiF (mp-1138) <1 1 0> <1 0 1> 0.018 258.7
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.020 158.9
GaP (mp-2490) <1 1 0> <1 0 1> 0.021 258.7
CaF2 (mp-2741) <1 1 0> <1 0 1> 0.022 258.7
KP(HO2)2 (mp-23959) <1 0 0> <0 0 1> 0.024 113.5
KP(HO2)2 (mp-23959) <0 1 0> <0 0 1> 0.028 227.0
Te2W (mp-22693) <0 1 1> <1 1 1> 0.028 235.3
Te2W (mp-22693) <1 0 0> <1 0 1> 0.030 295.6
C (mp-48) <1 1 0> <1 0 0> 0.033 233.2
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.036 188.3
NdGaO3 (mp-3196) <1 1 0> <1 0 1> 0.039 184.8
NaCl (mp-22862) <1 0 0> <0 0 1> 0.039 295.2
Te2Mo (mp-602) <0 0 1> <1 0 0> 0.040 87.5
LiGaO2 (mp-5854) <0 1 1> <0 0 1> 0.042 340.6
Ge (mp-32) <1 0 0> <0 0 1> 0.042 295.2
CdS (mp-672) <1 0 1> <1 0 0> 0.043 262.4
C (mp-66) <1 0 0> <0 0 1> 0.045 113.5
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.045 145.8
Fe3O4 (mp-19306) <1 0 0> <0 0 1> 0.046 295.2
Ge (mp-32) <1 1 0> <1 0 1> 0.047 332.6
NdGaO3 (mp-3196) <0 1 0> <1 0 1> 0.058 258.7
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.059 113.5
CdS (mp-672) <1 1 0> <1 1 0> 0.062 247.4
Mg (mp-153) <0 0 1> <0 0 1> 0.069 181.6
CaF2 (mp-2741) <1 0 0> <1 0 1> 0.073 184.8
NdGaO3 (mp-3196) <1 0 0> <1 0 1> 0.074 221.7
WSe2 (mp-1821) <1 0 1> <0 0 1> 0.074 204.3
BaTiO3 (mp-5986) <1 0 1> <1 0 1> 0.076 258.7
C (mp-48) <0 0 1> <0 0 1> 0.079 181.6
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.085 29.2
GaAs (mp-2534) <1 1 0> <1 0 1> 0.085 332.6
TeO2 (mp-2125) <1 1 0> <1 0 0> 0.086 291.5
SiC (mp-11714) <1 1 0> <1 0 0> 0.090 320.7
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.093 41.2
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.095 204.3
GaP (mp-2490) <1 0 0> <1 0 1> 0.095 184.8
WSe2 (mp-1821) <1 0 0> <0 0 1> 0.096 204.3
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.098 113.5
Ni (mp-23) <1 1 0> <1 1 0> 0.101 206.1
CsI (mp-614603) <1 0 0> <1 0 1> 0.104 184.8
YAlO3 (mp-3792) <1 1 1> <1 1 0> 0.105 123.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
97 49 107 0 0 0
49 97 107 0 0 0
107 107 288 0 0 0
0 0 0 58 0 0
0 0 0 0 58 0
0 0 0 0 0 34
Compliance Tensor Sij (10-12Pa-1)
18.1 -3 -5.6 0 0 0
-3 18.1 -5.6 0 0 0
-5.6 -5.6 7.6 0 0 0
0 0 0 17.1 0 0
0 0 0 0 17.1 0
0 0 0 0 0 29.1
Shear Modulus GV
45 GPa
Bulk Modulus KV
112 GPa
Shear Modulus GR
36 GPa
Bulk Modulus KR
65 GPa
Shear Modulus GVRH
40 GPa
Bulk Modulus KVRH
89 GPa
Elastic Anisotropy
2.02
Poisson's Ratio
0.30

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.00000 0.00000 0.00000
0.00000 0.00000 0.00000 0.00000 0.00000 0.00000
0.00000 0.00000 0.00000 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
0.00000 C/m2
Crystallographic Direction vmax
1.00000
0.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
4.81 0.00 0.00
0.00 4.81 0.00
0.00 0.00 4.51
Dielectric Tensor εij (total)
14.54 0.00 0.00
0.00 14.54 0.00
0.00 0.00 14.58
Polycrystalline dielectric constant εpoly
(electronic contribution)
1.57
Polycrystalline dielectric constant εpoly
(total)
1.57
Refractive Index n
1.25
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TaAl(WO4)2 (mvc-640) 0.5422 0.067 4
AlRe(WO4)2 (mvc-735) 0.5838 0.126 4
LiMn2OF5 (mp-764255) 0.5927 0.041 4
LiVOF3 (mp-764760) 0.5194 0.024 4
LiMn3(OF3)2 (mp-767084) 0.5599 0.016 4
VO2 (mvc-12077) 0.4426 0.079 2
TiO2 (mvc-12404) 0.4101 0.061 2
VO2 (mp-715553) 0.5079 0.071 2
TiO2 (mp-9173) 0.4068 0.059 2
TiO2 (mp-754769) 0.4296 0.052 2
VOF (mp-778746) 0.2670 0.000 3
FeOF (mp-762996) 0.1982 0.063 3
FeOF (mp-763016) 0.2424 0.062 3
FeOF (mp-763022) 0.2811 0.063 3
FeOF (mp-780817) 0.2010 0.062 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Fe: 5.3 eV
Pseudopotentials
VASP PAW: Fe_pv O F
Final Energy/Atom
-6.0065 eV
Corrected Energy
-85.8186 eV
-85.8186 eV = -72.0775 eV (uncorrected energy) - 10.9320 eV (MP Advanced Correction) - 2.8092 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)