Final Magnetic Moment11.398 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.595 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.784 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.59 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe3O4 + FeO |
Band Gap0.211 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 257.8 |
AlN (mp-661) | <1 1 0> | <1 -1 -1> | 248.0 |
KCl (mp-23193) | <1 1 1> | <0 1 -1> | 297.8 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 140.3 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 280.2 |
GaN (mp-804) | <1 1 0> | <0 1 -1> | 297.8 |
SiO2 (mp-6930) | <1 0 0> | <1 -1 -1> | 248.0 |
KCl (mp-23193) | <1 1 0> | <0 1 -1> | 297.8 |
TePb (mp-19717) | <1 1 1> | <0 1 -1> | 297.8 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 257.8 |
BN (mp-984) | <1 0 0> | <0 1 0> | 171.9 |
TePb (mp-19717) | <1 1 0> | <0 1 -1> | 297.8 |
LiNbO3 (mp-3731) | <1 1 0> | <0 1 0> | 257.8 |
LiGaO2 (mp-5854) | <0 0 1> | <1 -1 -1> | 248.0 |
SiC (mp-7631) | <0 0 1> | <0 1 -1> | 99.3 |
SiC (mp-7631) | <1 1 0> | <1 -1 -1> | 248.0 |
CdTe (mp-406) | <1 1 1> | <0 1 -1> | 297.8 |
SiC (mp-7631) | <1 0 0> | <0 1 1> | 140.3 |
LiTaO3 (mp-3666) | <1 1 0> | <0 1 0> | 257.8 |
LiTaO3 (mp-3666) | <1 1 1> | <0 1 0> | 257.8 |
TiO2 (mp-2657) | <0 0 1> | <0 1 -1> | 297.8 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 257.8 |
TiO2 (mp-2657) | <1 1 1> | <0 1 -1> | 297.8 |
C (mp-66) | <1 1 0> | <0 1 0> | 257.8 |
GdScO3 (mp-5690) | <1 1 1> | <1 0 0> | 280.2 |
TbScO3 (mp-31119) | <1 1 1> | <1 0 0> | 280.2 |
NdGaO3 (mp-3196) | <1 0 1> | <0 1 0> | 257.8 |
InSb (mp-20012) | <1 1 1> | <0 1 -1> | 297.8 |
SiC (mp-11714) | <0 0 1> | <0 1 -1> | 99.3 |
Ga2O3 (mp-886) | <1 0 1> | <0 1 1> | 140.3 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 0> | 280.2 |
MoSe2 (mp-1634) | <1 0 0> | <1 -1 -1> | 248.0 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 186.8 |
ZrO2 (mp-2858) | <0 1 1> | <1 0 0> | 280.2 |
WSe2 (mp-1821) | <1 0 0> | <1 -1 -1> | 248.0 |
ZrO2 (mp-2858) | <0 0 1> | <0 1 -1> | 297.8 |
ZrO2 (mp-2858) | <0 1 0> | <1 -1 -1> | 248.0 |
ZrO2 (mp-2858) | <1 1 0> | <0 1 -1> | 198.5 |
YAlO3 (mp-3792) | <0 1 0> | <0 1 -1> | 198.5 |
MgF2 (mp-1249) | <1 0 0> | <0 1 0> | 85.9 |
ZnO (mp-2133) | <1 0 1> | <1 0 0> | 280.2 |
SiC (mp-8062) | <1 0 0> | <0 1 0> | 171.9 |
CdWO4 (mp-19387) | <0 1 0> | <0 1 -1> | 297.8 |
Cu (mp-30) | <1 1 0> | <0 1 0> | 257.8 |
MgF2 (mp-1249) | <1 0 1> | <1 0 0> | 186.8 |
ZnO (mp-2133) | <1 1 0> | <0 1 -1> | 297.8 |
GaTe (mp-542812) | <0 1 0> | <0 1 -1> | 198.5 |
GaTe (mp-542812) | <1 1 0> | <0 1 -1> | 198.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li35(RuO4)12 (mp-757535) | 0.3178 | 0.000 | 3 |
Mn(Ni9O10)2 (mp-763814) | 0.3158 | 0.028 | 3 |
Li9Co9O17 (mp-735506) | 0.2614 | 0.122 | 3 |
Li11(NiO2)12 (mp-38676) | 0.2580 | 0.009 | 3 |
Li11(NiO2)12 (mp-698713) | 0.2062 | 0.009 | 3 |
NaLiMg30O31 (mp-1040127) | 0.1922 | 0.093 | 4 |
NaLiMg30O31 (mp-1040115) | 0.1872 | 0.093 | 4 |
NaLiMg30O31 (mp-1040107) | 0.1798 | 0.091 | 4 |
NaLiMg30O31 (mp-1040085) | 0.2026 | 0.089 | 4 |
Fe17O18 (mp-705424) | 0.2823 | 0.041 | 2 |
Fe38O39 (mp-705753) | 0.1508 | 0.071 | 2 |
Fe14O15 (mp-764417) | 0.3370 | 0.059 | 2 |
Ni15Cl16 (mp-1094137) | 0.3564 | 0.277 | 2 |
Ni15O16 (mp-705519) | 0.3489 | 0.038 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.7428 | 0.882 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Fe_pv O |
Final Energy/Atom-5.9378 eV |
Corrected Energy-542.5200 eV
-542.5200 eV = -421.5826 eV (uncorrected energy) - 95.6550 eV (MP Advanced Correction) - 25.2824 eV (MP Anion Correction)
|