Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.814 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.117 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.78 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCaSnO3 + Ca2SnO4 + La5Mn5O16 + Sn |
Band Gap0.668 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 1 0> | 142.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 130.9 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 320.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 196.4 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 274.5 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 219.4 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 44.0 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 109.7 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 308.2 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 224.2 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 88.0 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 219.4 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 98.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 32.7 |
GaAs (mp-2534) | <1 1 0> | <1 1 -1> | 190.5 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 352.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 163.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 130.9 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 176.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 32.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 54.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 -1> | 63.5 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 1> | 219.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 32.7 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 54.9 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 272.9 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 213.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 54.9 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 109.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 294.6 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 220.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 44.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 54.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 44.0 |
ZnSe (mp-1190) | <1 1 0> | <1 1 -1> | 190.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 32.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 44.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 32.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 360.1 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 274.5 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 329.1 |
CdS (mp-672) | <1 1 1> | <1 1 -1> | 254.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 98.2 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 163.7 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 176.1 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 294.6 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 280.3 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 142.6 |
Te2Mo (mp-602) | <1 0 0> | <1 0 -1> | 274.5 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 137.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaCrO3 (mp-24909) | 0.2293 | 0.056 | 3 |
PrFeO3 (mp-24995) | 0.2276 | 0.123 | 3 |
LaVO3 (mp-19350) | 0.1859 | 0.000 | 3 |
NdMnO3 (mp-565535) | 0.2108 | 0.287 | 3 |
LaMnO3 (mp-629046) | 0.2302 | 0.120 | 3 |
Ca2TiWO6 (mvc-5090) | 0.1811 | 0.081 | 4 |
Ca2CuWO6 (mvc-5004) | 0.1949 | 0.065 | 4 |
Ca2CoWO6 (mvc-10897) | 0.1924 | 0.000 | 4 |
Ca2FeMoO6 (mvc-16547) | 0.1924 | 0.195 | 4 |
Nd2MnCoO6 (mp-19336) | 0.1851 | 0.000 | 4 |
FeSb3 (mp-971669) | 0.7473 | 0.000 | 2 |
Pb3O4 (mp-636813) | 0.6498 | 0.038 | 2 |
Al2O3 (mp-642363) | 0.7395 | 0.280 | 2 |
CaNdTiMnO6 (mp-41742) | 0.1702 | 0.174 | 5 |
CaLaTaFeO6 (mvc-9005) | 0.1763 | 0.000 | 5 |
CaLaFeMoO6 (mvc-9015) | 0.1839 | 0.202 | 5 |
CaLaMnRuO6 (mp-690556) | 0.1862 | 0.080 | 5 |
CaNdTiMnO6 (mp-705449) | 0.1540 | 0.174 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Ca_sv La Mn_pv Sn_d O |
Final Energy/Atom-7.2023 eV |
Corrected Energy-155.8350 eV
-155.8350 eV = -144.0458 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 3.3617 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)