Final Magnetic Moment0.512 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.100 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.050 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.81 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLa3Ga5O12 + Mg(GaO2)2 + La4Ga2O9 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 207.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 138.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 207.8 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 280.3 |
SiO2 (mp-6930) | <1 1 1> | <1 -1 0> | 277.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 210.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 274.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 69.3 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 296.9 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 140.2 |
GaN (mp-804) | <0 0 1> | <1 1 -1> | 134.1 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 280.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 138.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 296.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 140.2 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 280.3 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 274.6 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 0> | 274.6 |
CdTe (mp-406) | <1 0 0> | <1 0 1> | 134.0 |
TeO2 (mp-2125) | <1 0 0> | <0 1 1> | 296.9 |
TeO2 (mp-2125) | <1 1 0> | <0 1 1> | 99.0 |
TiO2 (mp-2657) | <1 0 0> | <1 0 -1> | 275.1 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 207.8 |
GdScO3 (mp-5690) | <0 1 1> | <0 1 0> | 210.3 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 140.2 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 -1> | 275.1 |
GdScO3 (mp-5690) | <1 1 1> | <0 0 1> | 69.3 |
Mg (mp-153) | <0 0 1> | <1 -1 -1> | 279.2 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 280.3 |
C (mp-66) | <1 0 0> | <0 0 1> | 207.8 |
LaF3 (mp-905) | <1 0 1> | <1 0 0> | 274.6 |
GaP (mp-2490) | <1 0 0> | <0 1 0> | 210.3 |
GaP (mp-2490) | <1 1 0> | <0 1 1> | 296.9 |
TbScO3 (mp-31119) | <0 1 0> | <0 1 1> | 296.9 |
TbScO3 (mp-31119) | <0 1 1> | <0 1 0> | 210.3 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 0> | 140.2 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 -1> | 275.1 |
TbScO3 (mp-31119) | <1 1 1> | <0 0 1> | 69.3 |
Ni (mp-23) | <1 1 0> | <1 0 -1> | 275.1 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 -1> | 275.1 |
InSb (mp-20012) | <1 0 0> | <1 0 1> | 134.0 |
MoSe2 (mp-1634) | <1 1 0> | <0 1 0> | 280.3 |
NdGaO3 (mp-3196) | <0 1 0> | <0 1 1> | 296.9 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 207.8 |
NdGaO3 (mp-3196) | <1 1 1> | <0 0 1> | 69.3 |
Ga2O3 (mp-886) | <1 0 -1> | <0 1 1> | 198.0 |
Si (mp-149) | <1 0 0> | <0 0 1> | 207.8 |
Si (mp-149) | <1 1 0> | <0 1 1> | 296.9 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 277.1 |
ZrO2 (mp-2858) | <1 1 0> | <1 0 0> | 274.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaOsO3 (mp-998624) | 0.1817 | 0.015 | 3 |
CuAgF3 (mp-998422) | 0.1676 | 0.013 | 3 |
LaCoO3 (mp-561922) | 0.2395 | 0.011 | 3 |
LaGaO3 (mp-1078871) | 0.1532 | 0.039 | 3 |
CuAgF3 (mp-1099573) | 0.2018 | 0.013 | 3 |
La2ZnFeO6 (mvc-13418) | 0.1834 | 0.014 | 4 |
La2MnZnO6 (mvc-13688) | 0.2024 | 0.070 | 4 |
La2MgMnO6 (mvc-10946) | 0.1988 | 0.033 | 4 |
La2MgGeO6 (mp-11585) | 0.1818 | 0.016 | 4 |
La2MgMnO6 (mp-19406) | 0.1984 | 0.033 | 4 |
In2Ag (mp-760385) | 0.6875 | 0.096 | 2 |
Hf2Ge (mp-1072256) | 0.6891 | 0.622 | 2 |
CaLa9Ti5Cr5O30 (mp-694926) | 0.1642 | 0.063 | 5 |
Ca2La8Ti5Cr5O30 (mp-743953) | 0.1736 | 0.046 | 5 |
SrLa7TiGa7O24 (mp-720505) | 0.2644 | 0.015 | 5 |
SrLaMnRuO6 (mp-39239) | 0.2291 | 0.094 | 5 |
SrLaMnRuO6 (mp-690590) | 0.2363 | 0.094 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La Mg_pv Ga_d O |
Final Energy/Atom-7.2116 eV |
Corrected Energy-381.6486 eV
-381.6486 eV = -360.5799 eV (uncorrected energy) - 21.0687 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)