Final Magnetic Moment2.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.639 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.524 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.19 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRbHSO4 + RbP(HO2)2 |
Band Gap0.752 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 -1 0> | 286.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 199.8 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 266.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 244.8 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 203.9 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 203.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 219.1 |
BaF2 (mp-1029) | <1 1 1> | <1 1 0> | 203.9 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 221.5 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 133.2 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 203.9 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 333.1 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 219.1 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 333.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 146.0 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 219.1 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 203.9 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 292.1 |
KCl (mp-23193) | <1 1 1> | <1 1 0> | 203.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 -1> | 214.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 219.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 333.1 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 1> | 281.7 |
InAs (mp-20305) | <1 0 0> | <1 -1 0> | 191.2 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 219.1 |
InAs (mp-20305) | <1 1 1> | <1 1 0> | 203.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 333.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 257.0 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 333.1 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 292.1 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 257.0 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 292.1 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 292.1 |
Te2Mo (mp-602) | <0 0 1> | <0 1 -1> | 273.5 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 266.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 102.0 |
GaSe (mp-1943) | <0 0 1> | <1 1 -1> | 214.2 |
BN (mp-984) | <0 0 1> | <1 -1 0> | 191.2 |
BN (mp-984) | <1 0 0> | <0 0 1> | 257.0 |
BN (mp-984) | <1 0 1> | <0 1 0> | 199.8 |
BN (mp-984) | <1 1 1> | <0 1 -1> | 273.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 257.0 |
Bi2Se3 (mp-541837) | <1 0 1> | <1 0 -1> | 244.8 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 192.7 |
Al (mp-134) | <1 1 1> | <0 1 0> | 333.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 333.1 |
LiGaO2 (mp-5854) | <1 0 0> | <1 -1 0> | 286.8 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 219.1 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 -1> | 244.8 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 -1> | 163.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
H7NO6 (mp-626529) | 0.7214 | 0.032 | 3 |
H7NO6 (mp-626112) | 0.7453 | 0.037 | 3 |
Ag3I(NO3)2 (mp-653562) | 0.7184 | 0.234 | 4 |
H5C2NO3 (mp-738670) | 0.7098 | 0.131 | 4 |
H18Se3(NO3)4 (mp-708038) | 0.6968 | 0.455 | 4 |
H4CN5Cl (mp-696231) | 0.7367 | 0.109 | 4 |
KH(CN2)3 (mp-696886) | 0.7144 | 0.711 | 4 |
CaH16C4N8(ClO2)2 (mp-735603) | 0.6643 | 0.305 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv P H S O |
Final Energy/Atom-5.2746 eV |
Corrected Energy-170.8017 eV
-170.8017 eV = -158.2382 eV (uncorrected energy) - 12.5636 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)