Final Magnetic Moment1.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.503 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.557 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.72 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH8RuN3Cl5O + H4NCl + H2O + N2 + Ru |
Band Gap0.842 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 -1> | 288.3 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 234.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 234.7 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 288.3 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 234.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 234.7 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 312.9 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 156.4 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 -1> | 288.3 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 146.8 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 260.4 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 288.3 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 156.4 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 234.7 |
YVO4 (mp-19133) | <1 0 1> | <1 0 -1> | 288.3 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 146.8 |
BN (mp-984) | <0 0 1> | <1 0 0> | 234.7 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 0> | 151.9 |
MoS2 (mp-1434) | <1 1 0> | <1 0 0> | 234.7 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 -1> | 288.3 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 -1> | 96.1 |
TeO2 (mp-2125) | <0 1 1> | <1 0 -1> | 288.3 |
SiC (mp-7631) | <0 0 1> | <1 0 -1> | 288.3 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 260.4 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 234.7 |
C (mp-66) | <1 1 0> | <1 0 -1> | 288.3 |
GdScO3 (mp-5690) | <1 1 1> | <1 0 -1> | 288.3 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 234.7 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 234.7 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 234.7 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 78.2 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 78.2 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 234.7 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 156.4 |
LaF3 (mp-905) | <1 0 1> | <1 0 -1> | 288.3 |
PbS (mp-21276) | <1 1 1> | <1 0 0> | 312.9 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 234.7 |
InP (mp-20351) | <1 1 1> | <1 0 0> | 312.9 |
TbScO3 (mp-31119) | <1 1 1> | <1 0 -1> | 288.3 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 260.4 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 156.4 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 234.7 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 234.7 |
SiC (mp-11714) | <0 0 1> | <1 0 -1> | 288.3 |
Si (mp-149) | <1 0 0> | <1 0 0> | 234.7 |
Au (mp-81) | <1 1 0> | <1 0 1> | 146.8 |
WS2 (mp-224) | <1 1 0> | <1 1 0> | 151.9 |
ZrO2 (mp-2858) | <0 1 0> | <1 0 0> | 312.9 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 234.7 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 -1> | 288.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Si(H3C)2 (mp-978595) | 0.7465 | 0.056 | 3 |
Sb6S2O15 (mp-27229) | 0.6783 | 0.000 | 3 |
PH8N3O2 (mp-697683) | 0.7175 | 0.000 | 4 |
PH7N2O3 (mp-707905) | 0.7150 | 0.050 | 4 |
Si2H25C10N (mp-605056) | 0.6508 | 0.066 | 4 |
H8Se2N2O5 (mp-707226) | 0.7033 | 0.089 | 4 |
PH6(NO)2 (mp-706622) | 0.6820 | 0.015 | 4 |
HgH6I3NO (mp-976118) | 0.7387 | 0.017 | 5 |
Zn3P3H10C2NO13 (mp-709326) | 0.6619 | 0.250 | 6 |
Zn2P3H19C4(NO6)2 (mp-535004) | 0.7467 | 0.033 | 6 |
Zn4P3H10C2NO13 (mp-736581) | 0.6271 | 0.029 | 6 |
ZnGaP2H4NO8 (mp-721013) | 0.6783 | 0.009 | 6 |
RbLiH4S2(NO3)2 (mp-699447) | 0.7401 | 0.053 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: H Ru_pv N Cl O |
Final Energy/Atom-4.6744 eV |
Corrected Energy-201.9416 eV
-201.9416 eV = -196.3232 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)