Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.460 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.914 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa(HO)2 + Ca2SiO4 + CaF2 |
Band Gap2.956 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 265.0 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 249.7 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 198.7 |
AlN (mp-661) | <1 1 0> | <1 1 -1> | 271.3 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 302.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 300.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 316.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 225.3 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 249.7 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 251.9 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 117.1 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 242.9 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 251.9 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 150.2 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 105.7 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 316.9 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 225.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 -1> | 271.3 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 211.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 316.9 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 225.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 300.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 161.9 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 151.2 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 225.3 |
CdS (mp-672) | <1 0 1> | <1 0 -1> | 300.5 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 190.2 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 253.5 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 211.4 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 225.3 |
Te2W (mp-22693) | <0 1 1> | <0 1 1> | 242.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 253.5 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 316.9 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 201.5 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 265.0 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 265.0 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 198.7 |
BN (mp-984) | <1 0 1> | <1 1 -1> | 180.9 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 126.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 151.2 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 251.9 |
Al (mp-134) | <1 1 0> | <0 1 1> | 161.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 302.3 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 198.7 |
LiGaO2 (mp-5854) | <1 1 1> | <1 1 0> | 166.5 |
TeO2 (mp-2125) | <0 0 1> | <1 0 -1> | 300.5 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 316.9 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 190.2 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 302.3 |
C (mp-66) | <1 1 0> | <1 0 0> | 265.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
As5Pb3S10 (mp-667418) | 0.5962 | 0.133 | 3 |
Te2PdBr6 (mp-569830) | 0.6652 | 0.004 | 3 |
As9Pb7S20 (mp-646283) | 0.6734 | 0.029 | 3 |
As2Pb2S5 (mp-608653) | 0.6080 | 0.005 | 3 |
As5Pb3S10 (mp-773040) | 0.6824 | 0.081 | 3 |
KNa2AlH6 (mp-600151) | 0.7492 | 0.155 | 4 |
Y2BeAlBO7 (mp-686689) | 0.6693 | 0.278 | 5 |
LaZnCrBiO6 (mvc-9918) | 0.7314 | 0.203 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Si H O F |
Final Energy/Atom-6.1201 eV |
Corrected Energy-228.7152 eV
-228.7152 eV = -220.3232 eV (uncorrected energy) - 8.3920 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)