Final Magnetic Moment0.909 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.376 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.166 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.36 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa3PSO3 + H2O |
Band Gap0.793 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR32 [155] |
HallR 3 2" |
Point Group32 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 223.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 223.5 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 298.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 74.5 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 223.5 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 298.0 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 74.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 298.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 223.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 223.5 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 223.5 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 74.5 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 74.5 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 298.0 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 223.5 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 223.5 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 149.0 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 223.5 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 74.5 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 74.5 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 298.0 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 74.5 |
C (mp-48) | <1 0 1> | <0 0 1> | 298.0 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 298.0 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 149.0 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 223.5 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 223.5 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 298.0 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 149.0 |
SiC (mp-8062) | <1 1 1> | <0 0 1> | 298.0 |
Ge (mp-32) | <1 1 1> | <0 0 1> | 223.5 |
LiAlO2 (mp-3427) | <1 0 0> | <0 0 1> | 298.0 |
CaF2 (mp-2741) | <1 1 1> | <0 0 1> | 223.5 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 298.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Lu(HO)3 (mp-676145) | 0.7273 | 0.093 | 3 |
Al(HO)3 (mp-626481) | 0.6649 | 0.069 | 3 |
KH9O5 (mp-28196) | 0.7297 | 0.005 | 3 |
MoH4O5 (mp-744482) | 0.7234 | 0.143 | 3 |
Ag(H7O4)2 (mp-777775) | 0.6427 | 0.069 | 3 |
MgH12SO10 (mp-696407) | 0.6539 | 0.451 | 4 |
SnH6Cl4O3 (mp-705479) | 0.5419 | 0.001 | 4 |
NaH2SO4 (mp-721314) | 0.6361 | 0.032 | 4 |
FeH6SO6 (mp-744930) | 0.6674 | 0.151 | 4 |
InH5(NF)2 (mp-733932) | 0.6714 | 0.000 | 4 |
Hg2H2C2NCl5 (mp-736665) | 0.6282 | 0.732 | 5 |
KV5Zn(H8O11)2 (mp-744332) | 0.6836 | 0.325 | 5 |
CoH19S3N5O11 (mp-745100) | 0.7073 | 0.077 | 5 |
CoH5SeClO5 (mp-776636) | 0.7066 | 0.008 | 5 |
Co2H21S3(NO2)6 (mp-744397) | 0.5618 | 0.142 | 5 |
Na4H20RuS4(NO9)2 (mp-720279) | 0.6370 | 0.082 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv P H S O |
Final Energy/Atom-4.8825 eV |
Corrected Energy-452.0553 eV
-452.0553 eV = -429.6597 eV (uncorrected energy) - 22.3956 eV (MP Anion Correction)
|