Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.435 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.007 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.26 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNd3Si6N11 + BaSiN2 + NdBN2 + BaN2 + NdN |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP6 [174] |
HallP 6 |
Point Group6 |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 202.7 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 67.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 202.7 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 135.1 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 117.0 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 117.0 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 270.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 135.1 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 234.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 135.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 270.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 131.8 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 202.7 |
BN (mp-984) | <1 0 1> | <1 0 0> | 202.7 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 135.1 |
MoS2 (mp-1434) | <1 1 0> | <1 1 0> | 117.0 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 131.8 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 234.0 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 202.7 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 202.7 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 67.6 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 202.7 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 135.1 |
Mg (mp-153) | <1 1 0> | <1 1 0> | 117.0 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 270.2 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 135.1 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 1 0> | 234.0 |
C (mp-66) | <1 0 0> | <1 0 0> | 270.2 |
C (mp-66) | <1 1 0> | <1 0 0> | 270.2 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 270.2 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 1 0> | 234.0 |
LaF3 (mp-905) | <1 1 0> | <1 0 0> | 270.2 |
LaF3 (mp-905) | <1 1 1> | <1 0 0> | 202.7 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 270.2 |
NdGaO3 (mp-3196) | <0 1 1> | <1 0 0> | 270.2 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 202.7 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 270.2 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 0> | 135.1 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 270.2 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 270.2 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 263.6 |
Si (mp-149) | <1 0 0> | <1 1 0> | 117.0 |
Au (mp-81) | <1 0 0> | <0 0 1> | 263.6 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 202.7 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 270.2 |
C (mp-48) | <0 0 1> | <0 0 1> | 131.8 |
C (mp-48) | <1 0 1> | <1 0 0> | 202.7 |
WSe2 (mp-1821) | <1 0 0> | <1 0 0> | 202.7 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 202.7 |
WS2 (mp-224) | <1 1 0> | <1 1 0> | 234.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Nd_3 Si B N |
Final Energy/Atom-7.8580 eV |
Corrected Energy-400.7558 eV
-400.7558 eV = -400.7558 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)