Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.456 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.864 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToScF3 |
Band Gap1.842 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC222 [21] |
HallC 2 2 |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 218.1 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 218.1 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 1> | 256.6 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 141.0 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 237.9 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 225.3 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 105.8 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 112.2 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 85.5 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 261.9 |
CeO2 (mp-20194) | <1 0 0> | <1 1 1> | 187.0 |
GaAs (mp-2534) | <1 1 1> | <1 0 1> | 282.0 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 190.8 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 136.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 193.7 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 105.8 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 218.1 |
GaN (mp-804) | <1 0 0> | <1 1 1> | 149.6 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 175.3 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 112.7 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 246.8 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 112.7 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 100.2 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 187.8 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 176.3 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 105.8 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 112.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 62.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 85.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 212.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 136.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 212.8 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 190.8 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 136.3 |
ZnSe (mp-1190) | <1 1 1> | <1 0 1> | 282.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 70.5 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 141.0 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 75.1 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 162.7 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 51.2 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 237.9 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 70.5 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 141.0 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 54.5 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 112.7 |
Te2W (mp-22693) | <1 1 0> | <1 0 1> | 105.8 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 204.9 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 262.9 |
TePb (mp-19717) | <1 1 0> | <0 1 1> | 256.6 |
TePb (mp-19717) | <1 1 1> | <1 1 0> | 218.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba(NdS2)2 (mp-34459) | 0.7065 | 0.052 | 3 |
Tb2PbS4 (mp-675645) | 0.7023 | 0.062 | 3 |
Sr(YbS2)2 (mp-675445) | 0.6960 | 0.287 | 3 |
Dy2PbS4 (mp-675209) | 0.6991 | 0.068 | 3 |
Ba(LaS2)2 (mp-33615) | 0.7058 | 0.013 | 3 |
BiO2 (mvc-15971) | 0.6468 | 0.565 | 2 |
La5S8 (mp-32640) | 0.7060 | 0.096 | 2 |
Ni3Se2 (mp-2056) | 0.7205 | 0.000 | 2 |
Ni3S2 (mp-362) | 0.7420 | 0.000 | 2 |
GaAu (mp-30379) | 0.7219 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sc_sv F |
Final Energy/Atom-6.1048 eV |
Corrected Energy-24.4190 eV
-24.4190 eV = -24.4190 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)