Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.116 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.125 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.78 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSOF2 + SbH3OF6 + SbF4 + CO2 + S(OF)2 + CF4 |
Band Gap4.512 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 171.7 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 171.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 105.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 111.7 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 210.3 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 210.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 111.7 |
LiNbO3 (mp-3731) | <1 1 1> | <0 0 1> | 257.6 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 257.6 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 105.1 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 210.3 |
Al (mp-134) | <1 1 1> | <1 0 -1> | 111.7 |
LiTaO3 (mp-3666) | <1 1 1> | <0 0 1> | 257.6 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 105.1 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 -1> | 111.7 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 105.1 |
LaF3 (mp-905) | <1 0 1> | <1 0 0> | 210.3 |
GdScO3 (mp-5690) | <1 1 1> | <1 0 0> | 210.3 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 105.1 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 -1> | 111.7 |
TbScO3 (mp-31119) | <1 1 1> | <1 0 0> | 210.3 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 271.3 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 105.1 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 85.9 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 271.3 |
NdGaO3 (mp-3196) | <0 1 1> | <1 0 0> | 105.1 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 -1> | 111.7 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 0> | 210.3 |
MoSe2 (mp-1634) | <0 0 1> | <0 1 0> | 180.9 |
WS2 (mp-224) | <0 0 1> | <1 0 0> | 105.1 |
C (mp-48) | <1 0 0> | <0 1 0> | 271.3 |
C (mp-48) | <1 1 0> | <0 1 0> | 271.3 |
C (mp-48) | <1 1 1> | <0 1 0> | 271.3 |
WSe2 (mp-1821) | <0 0 1> | <0 1 0> | 180.9 |
CdWO4 (mp-19387) | <0 1 0> | <0 1 0> | 271.3 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 257.6 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 257.6 |
TiO2 (mp-390) | <1 1 0> | <1 0 0> | 105.1 |
ZnO (mp-2133) | <0 0 1> | <1 0 -1> | 111.7 |
ZnO (mp-2133) | <1 0 0> | <1 0 0> | 105.1 |
SrTiO3 (mp-4651) | <1 0 1> | <1 0 0> | 105.1 |
SrTiO3 (mp-4651) | <1 1 1> | <1 0 0> | 210.3 |
Al2O3 (mp-1143) | <1 0 0> | <0 0 1> | 257.6 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 -1> | 223.5 |
Fe2O3 (mp-24972) | <1 0 1> | <1 0 -1> | 223.5 |
TiO2 (mp-390) | <1 0 0> | <1 0 -1> | 111.7 |
TiO2 (mp-390) | <1 0 1> | <0 1 0> | 271.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ta2H4O7 (mp-625957) | 0.6849 | 0.038 | 3 |
Re2H4O9 (mp-625238) | 0.7115 | 0.026 | 3 |
MoH4O5 (mp-744482) | 0.7464 | 0.143 | 3 |
Re2H4O9 (mp-625142) | 0.7387 | 0.111 | 3 |
ScH3(ClO5)2 (mp-756748) | 0.6386 | 0.000 | 4 |
SnH10Cl4O5 (mp-766259) | 0.7130 | 0.001 | 4 |
Li2Sn(H5O4)2 (mp-703343) | 0.7000 | 0.007 | 4 |
TiPCl7O (mp-559493) | 0.6839 | 0.000 | 4 |
ZrP2NCl11 (mp-570966) | 0.6744 | 0.000 | 4 |
CoPH6O6F (mp-743618) | 0.7199 | 0.007 | 5 |
Sb6H3CCl13O10 (mp-708066) | 0.7009 | 0.116 | 5 |
MnH12S2(NO5)2 (mp-849529) | 0.5856 | 0.155 | 5 |
CrH12N3(OF2)3 (mp-745188) | 0.6525 | 0.381 | 5 |
SbH32C8N4Cl7 (mp-708994) | 0.7019 | 0.066 | 5 |
SiH21C6N2OF5 (mp-849790) | 0.6753 | 0.118 | 6 |
CoMo8H36C8(NO16)2 (mp-745098) | 0.6560 | 0.196 | 6 |
NaH3C4S4(OF)12 (mp-709432) | 0.5853 | 0.169 | 6 |
As3H9RhC3(ClO)3 (mp-573080) | 0.6899 | 0.166 | 6 |
AsH3CNOF9 (mp-697077) | 0.7039 | 0.112 | 6 |
SbTe7SXeCl(OF4)9 (mp-560359) | 0.7183 | 0.043 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sb H C S O F |
Final Energy/Atom-5.0603 eV |
Corrected Energy-328.6602 eV
Uncorrected energy = -303.6202 eV
Composition-based energy adjustment (-0.503 eV/atom x 4.0 atoms) = -2.0120 eV
Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV
Composition-based energy adjustment (-0.462 eV/atom x 32.0 atoms) = -14.7840 eV
Corrected energy = -328.6602 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)