Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.353 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.95 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap7.881 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 174.6 |
LaAlO3 (mp-2920) | <1 0 0> | <1 -1 1> | 284.0 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 312.2 |
AlN (mp-661) | <0 0 1> | <1 0 -1> | 133.8 |
AlN (mp-661) | <1 0 0> | <0 1 -1> | 188.9 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 231.1 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 209.0 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 135.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 206.7 |
CeO2 (mp-20194) | <1 1 0> | <1 1 -1> | 254.8 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 298.6 |
GaAs (mp-2534) | <1 1 0> | <0 1 -1> | 188.9 |
BaF2 (mp-1029) | <1 0 0> | <1 -1 0> | 193.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 223.0 |
GaN (mp-804) | <0 0 1> | <0 1 -1> | 226.7 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 51.7 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 178.4 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 310.1 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 206.7 |
SiO2 (mp-6930) | <0 0 1> | <1 -1 0> | 290.8 |
SiO2 (mp-6930) | <1 0 0> | <1 -1 0> | 193.9 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 209.0 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 238.9 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 209.0 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 328.4 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 223.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 258.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 261.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 271.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 -1 0> | 242.3 |
InAs (mp-20305) | <1 0 0> | <1 -1 0> | 193.9 |
CdS (mp-672) | <0 0 1> | <1 -1 -1> | 281.3 |
CdS (mp-672) | <1 0 1> | <0 1 -1> | 188.9 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 149.3 |
YVO4 (mp-19133) | <1 1 0> | <0 1 -1> | 264.5 |
YVO4 (mp-19133) | <1 1 1> | <1 1 1> | 249.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 -1> | 188.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 -1> | 188.9 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 328.4 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 203.7 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 223.0 |
InAs (mp-20305) | <1 1 1> | <1 -1 -1> | 337.6 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 192.6 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 298.6 |
ZnSe (mp-1190) | <1 1 0> | <0 1 -1> | 188.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 149.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 -1> | 188.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 298.6 |
GaSe (mp-1943) | <1 0 0> | <1 -1 0> | 193.9 |
CdS (mp-672) | <1 0 0> | <0 1 -1> | 264.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
1.82 | 0.05 | -0.01 |
0.05 | 1.78 | 0.02 |
-0.01 | 0.02 | 1.90 |
Dielectric Tensor εij (total) |
||
---|---|---|
4.17 | 0.56 | 0.02 |
0.56 | 3.47 | 0.08 |
0.02 | 0.08 | 5.30 |
Polycrystalline dielectric constant
εpoly∞
1.83
|
Polycrystalline dielectric constant
εpoly
4.31
|
Refractive Index n1.35 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
H12Cl2O13 (mp-720382) | 0.4713 | 0.005 | 3 |
H3ClO5 (mp-625175) | 0.5023 | 0.004 | 3 |
H4SO5 (mp-626172) | 0.4905 | 0.017 | 3 |
H3ClO5 (mp-27694) | 0.5446 | 0.000 | 3 |
H4SO5 (mp-626229) | 0.5141 | 0.029 | 3 |
BH2OF3 (mp-707009) | 0.6889 | 0.000 | 4 |
KH5S2O9 (mp-541415) | 0.6579 | 0.000 | 4 |
P3H11N4O9 (mp-695955) | 0.6781 | 0.084 | 4 |
H3SO4F (mp-24463) | 0.6828 | 0.000 | 4 |
P2H10N2O7 (mp-740735) | 0.7089 | 0.223 | 4 |
CrN2 (mp-1016063) | 0.6696 | 0.438 | 2 |
P2O5 (mp-689684) | 0.6274 | 0.743 | 2 |
H3CSO4F3 (mp-24357) | 0.5303 | 0.133 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: B H O F |
Final Energy/Atom-5.2785 eV |
Corrected Energy-96.4180 eV
-96.4180 eV = -95.0134 eV (uncorrected energy) - 1.4046 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)