Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.568 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.025 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.38 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTlAgAs2PbS5 |
Band Gap1.107 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 247.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 185.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 308.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 308.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 308.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 247.1 |
BN (mp-984) | <1 0 0> | <0 0 1> | 247.1 |
Al (mp-134) | <1 0 0> | <0 0 1> | 308.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 247.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 247.1 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 308.8 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 308.8 |
C (mp-66) | <1 0 0> | <0 0 1> | 308.8 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 308.8 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 185.3 |
C (mp-66) | <1 1 0> | <0 0 1> | 308.8 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 308.8 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 308.8 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 308.8 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 247.1 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 308.8 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 308.8 |
Au (mp-81) | <1 0 0> | <0 0 1> | 308.8 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 308.8 |
C (mp-48) | <0 0 1> | <0 0 1> | 185.3 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 308.8 |
ZrO2 (mp-2858) | <1 0 1> | <0 0 1> | 308.8 |
ZrO2 (mp-2858) | <1 1 -1> | <0 0 1> | 185.3 |
ZrO2 (mp-2858) | <1 1 0> | <0 0 1> | 308.8 |
ZrO2 (mp-2858) | <1 1 1> | <0 0 1> | 308.8 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 308.8 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 308.8 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 308.8 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 308.8 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 185.3 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 308.8 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 308.8 |
GaTe (mp-542812) | <0 0 1> | <0 0 1> | 308.8 |
GaTe (mp-542812) | <1 0 -1> | <0 0 1> | 308.8 |
LiAlO2 (mp-3427) | <1 0 1> | <0 0 1> | 308.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tl_d Ag As Pb_d S |
Final Energy/Atom-4.1269 eV |
Corrected Energy-445.8640 eV
-445.8640 eV = -412.6910 eV (uncorrected energy) - 33.1730 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)