Final Magnetic Moment-0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-1.204 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.029 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.66 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBe3N2 |
Band Gap3.328 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 175.7 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 143.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 217.8 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 111.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 140.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 91.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 182.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 267.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 147.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 49.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 166.9 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 139.1 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 175.7 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 192.7 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 196.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 28.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 231.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 77.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 231.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 210.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 21.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 192.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 35.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 333.8 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 105.4 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 200.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 217.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 210.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 361.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 140.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 55.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 240.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 189.7 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 315.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 63.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 166.9 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 139.1 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 175.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 111.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 112.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 28.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 63.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 231.9 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 231.9 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 252.9 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 200.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 84.3 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 114.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 28.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 217.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiFeOF2 (mp-853231) | 0.3455 | 0.087 | 4 |
Zn3N2 (mp-754553) | 0.2413 | 0.011 | 2 |
Al2O3 (mp-755483) | 0.6551 | 0.091 | 2 |
AlCuO3 (mvc-15945) | 0.1702 | 0.188 | 3 |
YSnO3 (mvc-13971) | 0.0721 | 0.190 | 3 |
YMoO3 (mvc-3559) | 0.1258 | 0.198 | 3 |
MnAlO3 (mvc-15992) | 0.1660 | 0.271 | 3 |
YLuO3 (mp-754226) | 0.0923 | 0.073 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points20 |
U Values-- |
PseudopotentialsVASP PAW: Be_sv N |
Final Energy/Atom-6.6224 eV |
Corrected Energy-66.2241 eV
-66.2241 eV = -66.2241 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)