material

ScCuS2

ID:

mp-6980

DOI:

10.17188/1285273


Tags: Copper(I) scandium sulfide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.614 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.91 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.918 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3m1 [156]
Hall
P 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 15298 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ni (mp-23) <1 1 1> <0 0 1> 0.000 85.3
Cu (mp-30) <1 1 1> <0 0 1> 0.001 158.4
CdWO4 (mp-19387) <1 0 0> <1 1 0> 0.001 156.3
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.002 158.4
PbS (mp-21276) <1 0 0> <1 0 0> 0.003 180.5
CdS (mp-672) <1 0 0> <1 0 1> 0.007 230.8
DyScO3 (mp-31120) <0 1 0> <0 0 1> 0.009 304.6
ZrO2 (mp-2858) <1 1 -1> <1 1 0> 0.011 273.5
AlN (mp-661) <0 0 1> <0 0 1> 0.013 109.7
GaP (mp-2490) <1 1 1> <0 0 1> 0.017 158.4
Ge (mp-32) <1 1 1> <0 0 1> 0.022 231.5
Al (mp-134) <1 1 1> <0 0 1> 0.022 85.3
YAlO3 (mp-3792) <0 1 0> <0 0 1> 0.038 195.0
BN (mp-984) <0 0 1> <0 0 1> 0.050 48.7
C (mp-48) <0 0 1> <0 0 1> 0.051 36.6
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.058 158.4
Ge3(BiO3)4 (mp-23560) <1 1 1> <0 0 1> 0.058 195.0
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.059 85.3
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.060 48.7
SiO2 (mp-6930) <1 1 1> <1 1 0> 0.061 156.3
GaAs (mp-2534) <1 1 1> <0 0 1> 0.063 231.5
LiF (mp-1138) <1 1 0> <1 1 1> 0.078 163.7
ZrO2 (mp-2858) <1 1 1> <0 0 1> 0.080 255.9
Cu (mp-30) <1 1 0> <1 0 1> 0.085 128.2
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.087 255.9
InSb (mp-20012) <1 1 1> <0 0 1> 0.089 231.5
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.093 195.0
YAlO3 (mp-3792) <1 1 1> <1 0 0> 0.096 315.8
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.100 231.5
LiGaO2 (mp-5854) <1 0 1> <0 0 1> 0.101 134.0
CdTe (mp-406) <1 1 1> <0 0 1> 0.107 231.5
YVO4 (mp-19133) <1 1 1> <1 0 0> 0.108 248.2
NaCl (mp-22862) <1 1 0> <0 0 1> 0.113 182.8
LaAlO3 (mp-2920) <0 0 1> <1 0 0> 0.124 225.6
Al (mp-134) <1 1 0> <1 1 1> 0.131 163.7
C (mp-66) <1 1 0> <1 0 1> 0.134 128.2
SiO2 (mp-6930) <1 0 1> <1 1 1> 0.139 245.6
DyScO3 (mp-31120) <1 0 0> <0 0 1> 0.140 182.8
LiF (mp-1138) <1 1 1> <0 0 1> 0.141 85.3
C (mp-48) <1 0 1> <1 0 0> 0.142 180.5
GaN (mp-804) <1 0 1> <1 0 0> 0.145 135.4
BaF2 (mp-1029) <1 1 0> <1 0 1> 0.149 282.1
BN (mp-984) <1 1 1> <0 0 1> 0.154 207.2
SiC (mp-7631) <0 0 1> <0 0 1> 0.159 109.7
TiO2 (mp-390) <1 0 1> <1 0 0> 0.163 157.9
InP (mp-20351) <1 0 0> <1 0 0> 0.166 180.5
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.166 361.0
Al2O3 (mp-1143) <1 0 0> <0 0 1> 0.168 255.9
TiO2 (mp-2657) <1 1 0> <1 1 0> 0.168 39.1
SiC (mp-11714) <0 0 1> <0 0 1> 0.169 109.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
145 56 53 8 0 0
56 145 53 -8 0 0
53 53 148 0 0 0
8 -8 0 30 0 0
0 0 0 0 30 8
0 0 0 0 8 45
Compliance Tensor Sij (10-12Pa-1)
8.9 -2.8 -2.2 -3 0 0
-2.8 8.9 -2.2 3 0 0
-2.2 -2.2 8.4 0 0 0
-3 3 0 35.2 0 0
0 0 0 0 35.2 -6
0 0 0 0 -6 23.4
Shear Modulus GV
39 GPa
Bulk Modulus KV
84 GPa
Shear Modulus GR
36 GPa
Bulk Modulus KR
84 GPa
Shear Modulus GVRH
38 GPa
Bulk Modulus KVRH
84 GPa
Elastic Anisotropy
0.43
Poisson's Ratio
0.31

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.00000 -0.31188 -0.42900
-0.42900 0.42900 0.00000 -0.31188 0.00000 0.00000
-0.31846 -0.31846 -0.22302 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
0.68217 C/m2
Crystallographic Direction vmax
0.00000
1.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
10.58 -0.00 0.00
-0.00 10.58 0.00
0.00 0.00 10.41
Dielectric Tensor εij (total)
24.46 -0.00 0.00
-0.00 24.46 -0.00
0.00 -0.00 13.30
Polycrystalline dielectric constant εpoly
(electronic contribution)
10.52
Polycrystalline dielectric constant εpoly
(total)
20.74
Refractive Index n
3.24
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TmCuSe2 (mp-36209) 0.2657 0.011 3
LuCuSe2 (mp-677241) 0.3421 0.015 3
YCuSe2 (mp-675902) 0.2800 0.009 3
LuCuS2 (mp-1001780) 0.1078 0.000 3
LiMnTe2 (mp-12681) 0.3180 0.121 3
Li2MnV3O8 (mp-775327) 0.5391 0.008 4
Li2Ti3CoO8 (mp-775110) 0.5481 0.061 4
Li2CoGe3O8 (mp-769597) 0.5506 0.000 4
Li2VCo3O8 (mp-761729) 0.5258 0.036 4
ScAlCO (mp-1080747) 0.2285 0.000 4
Mn3O4 (mp-566607) 0.6606 0.000 2
Mn3O4 (mp-18759) 0.6574 0.000 2
Mn3N4 (mp-1080204) 0.6383 0.172 2
FeO2 (mp-1097003) 0.6522 1.147 2
Re3N4 (mp-1080201) 0.6314 0.110 2
Li4V2Cr3Fe3O16 (mp-770523) 0.5620 0.264 5
Li4Nb2V3Ni3O16 (mp-777087) 0.5720 0.024 5
Li4V2Co3Cu3O16 (mp-763156) 0.5402 0.088 5
Li4V2Co3Ni3O16 (mp-763125) 0.5749 0.119 5
Li4V2Cr3Co3O16 (mp-767986) 0.5717 0.130 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sc_sv Cu_pv S
Final Energy/Atom
-5.9580 eV
Corrected Energy
-24.8381 eV
Uncorrected energy = -23.8321 eV Composition-based energy adjustment (-0.503 eV/atom x 2.0 atoms) = -1.0060 eV Corrected energy = -24.8381 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 15298
Submitted by
User remarks:
  • Copper(I) scandium sulfide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)