Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.973 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.077 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH4NF + H3OF + H4C + SnF2 + C |
Band Gap4.728 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 -1> | 285.8 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 243.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 303.7 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 243.0 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 285.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 303.7 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 153.1 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 243.0 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 303.7 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 303.7 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 -1> | 285.8 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 243.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 213.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 303.7 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 60.7 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 149.3 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 213.9 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 303.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 285.8 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 95.3 |
YVO4 (mp-19133) | <1 0 1> | <1 0 -1> | 285.8 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 219.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 285.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 219.1 |
BN (mp-984) | <1 0 0> | <1 0 0> | 303.7 |
BN (mp-984) | <1 1 1> | <1 0 0> | 243.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 60.7 |
Al (mp-134) | <1 0 0> | <0 1 0> | 213.9 |
Al (mp-134) | <1 1 0> | <1 0 0> | 303.7 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 303.7 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 -1> | 285.8 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 182.2 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 -1> | 95.3 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 219.1 |
TeO2 (mp-2125) | <0 1 1> | <0 1 1> | 153.1 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 303.7 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 303.7 |
TiO2 (mp-2657) | <1 0 1> | <0 1 1> | 153.1 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <1 0 -1> | 190.5 |
C (mp-66) | <1 0 0> | <1 0 0> | 182.2 |
C (mp-66) | <1 1 0> | <0 0 1> | 109.5 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 182.2 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 243.0 |
GdScO3 (mp-5690) | <1 1 1> | <1 0 -1> | 285.8 |
Mg (mp-153) | <1 0 0> | <1 1 1> | 183.7 |
Mg (mp-153) | <1 1 1> | <0 1 1> | 153.1 |
LaF3 (mp-905) | <0 0 1> | <1 0 0> | 182.2 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 109.5 |
LaF3 (mp-905) | <1 0 1> | <1 0 -1> | 285.8 |
LaF3 (mp-905) | <1 1 0> | <1 0 0> | 182.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SbAs2Cl13 (mp-27786) | 0.7219 | 0.000 | 3 |
Fe3P2H3O11 (mp-744206) | 0.7086 | 0.449 | 4 |
MgH8(ClO6)2 (mp-989229) | 0.6692 | 0.009 | 4 |
MgP2H12O11 (mp-722397) | 0.6670 | 0.028 | 4 |
AlH15(NF)6 (mp-541900) | 0.6769 | 0.117 | 4 |
As2H3CF9 (mp-556083) | 0.5716 | 0.171 | 4 |
CoPH21N5O7 (mp-775736) | 0.6564 | 0.010 | 5 |
AsH5COF6 (mp-557908) | 0.5289 | 0.163 | 5 |
FeH12C2N2F5 (mp-565741) | 0.5390 | 0.139 | 5 |
CoH18C4N7O8 (mp-600278) | 0.5494 | 0.399 | 5 |
MnH10S2(NO2)4 (mp-566172) | 0.6309 | 0.073 | 5 |
SiH21C6N2OF5 (mp-849790) | 0.5903 | 0.118 | 6 |
FeH12C2S2(O2F)6 (mp-743577) | 0.6214 | 0.183 | 6 |
NiH44C12N8(ClO5)2 (mp-746343) | 0.4691 | 0.148 | 6 |
LiH8C2S2NO5 (mp-605006) | 0.5722 | 0.196 | 6 |
VH12C2S2(O2F)6 (mp-744032) | 0.6212 | 0.151 | 6 |
H18RuC6S3N3ClO3 (mp-706304) | 0.6764 | 0.292 | 7 |
NaAgH16C4S4(NO5)2 (mp-605018) | 0.5653 | 0.215 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sn_d H C N O F |
Final Energy/Atom-5.1197 eV |
Corrected Energy-214.0536 eV
Uncorrected energy = -209.9076 eV
Composition-based energy adjustment (-0.687 eV/atom x 2.0 atoms) = -1.3740 eV
Composition-based energy adjustment (-0.462 eV/atom x 6.0 atoms) = -2.7720 eV
Corrected energy = -214.0536 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)