Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.758 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.042 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.88 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH4C + H4NCl + CdH4NCl3 + C |
Band Gap3.438 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmce [64] |
Hall-C 2bc 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 284.6 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 284.6 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 284.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 170.8 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 159.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 284.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 170.8 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 341.5 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 341.5 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 284.6 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 227.7 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 227.7 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 284.6 |
BN (mp-984) | <1 0 0> | <0 1 0> | 56.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 284.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 170.8 |
BN (mp-984) | <0 0 1> | <0 1 0> | 284.6 |
BN (mp-984) | <1 1 0> | <0 1 0> | 227.7 |
Al (mp-134) | <1 0 0> | <0 1 0> | 284.6 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 148.9 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 284.6 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 170.8 |
CdTe (mp-406) | <1 0 0> | <0 1 0> | 227.7 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 284.6 |
SiC (mp-7631) | <1 0 0> | <0 1 0> | 227.7 |
SiC (mp-7631) | <1 0 1> | <0 1 0> | 227.7 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 0> | 284.6 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 0> | 284.6 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 284.6 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 284.6 |
MgO (mp-1265) | <1 1 1> | <0 1 0> | 284.6 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 341.5 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 1 0> | 113.8 |
C (mp-66) | <1 0 0> | <0 1 0> | 113.8 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 0> | 284.6 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 170.8 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 0> | 227.7 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 1 0> | 227.7 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 1 0> | 113.8 |
LaF3 (mp-905) | <1 1 0> | <0 1 0> | 284.6 |
GaP (mp-2490) | <1 0 0> | <0 1 0> | 284.6 |
LaF3 (mp-905) | <1 0 0> | <1 1 0> | 159.4 |
PbS (mp-21276) | <1 0 0> | <0 1 0> | 284.6 |
TbScO3 (mp-31119) | <0 0 1> | <0 1 0> | 284.6 |
InP (mp-20351) | <1 0 0> | <0 1 0> | 284.6 |
TbScO3 (mp-31119) | <0 1 0> | <0 1 0> | 170.8 |
InSb (mp-20012) | <1 0 0> | <0 1 0> | 227.7 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 0> | 284.6 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 284.6 |
NdGaO3 (mp-3196) | <0 0 1> | <0 1 0> | 284.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TePCl9 (mp-644827) | 0.7472 | 0.000 | 3 |
AlH6N2Cl3 (mp-740718) | 0.7364 | 0.000 | 4 |
ZnH12N3Cl5 (mp-723044) | 0.7306 | 0.000 | 4 |
SbCSF11 (mp-558893) | 0.7284 | 0.069 | 4 |
SbPOF8 (mp-560310) | 0.7329 | 0.000 | 4 |
AsCSF11 (mp-561235) | 0.6729 | 0.092 | 4 |
Re2O7 (mp-1016092) | 0.7319 | 0.000 | 2 |
MnH8C2NCl3 (mp-567451) | 0.4409 | 0.194 | 5 |
CdH8C2NCl3 (mp-570587) | 0.4481 | 0.062 | 5 |
MnH12C2(NCl2)2 (mp-698417) | 0.2073 | 0.140 | 5 |
SnH6CI3N (mp-1094059) | 0.4505 | 0.032 | 5 |
H6PbCBr3N (mp-1096997) | 0.4131 | 0.032 | 5 |
SiH21C6N2OF5 (mp-849790) | 0.5950 | 0.118 | 6 |
CoH14C3NCl3O2 (mp-600527) | 0.7025 | 0.082 | 6 |
NiH14C3NCl3O2 (mp-600519) | 0.7058 | 0.090 | 6 |
H12OsC4N(OF)3 (mp-738695) | 0.6711 | 0.330 | 6 |
AsC4S2Cl2O2F13 (mp-560424) | 0.6336 | 0.226 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cd H C N Cl |
Final Energy/Atom-4.5274 eV |
Corrected Energy-195.0610 eV
Uncorrected energy = -190.1490 eV
Composition-based energy adjustment (-0.614 eV/atom x 8.0 atoms) = -4.9120 eV
Corrected energy = -195.0610 eV
|