Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.015 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.003 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.43 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToP2H16N4O7 + PH8N2O3F + H9C6N11 + H4NF + PHN2 |
Band Gap4.935 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
YVO4 (mp-19133) | <0 0 1> | <1 0 1> | 160.5 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 93.5 |
YVO4 (mp-19133) | <1 0 1> | <1 0 -1> | 280.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 98.2 |
BN (mp-984) | <1 0 0> | <1 0 0> | 174.6 |
MoS2 (mp-1434) | <0 0 1> | <1 0 -1> | 280.5 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 294.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 294.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 294.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 196.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 294.5 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 -1> | 280.5 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 -1> | 93.5 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 294.5 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 187.0 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 160.5 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 294.5 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <1 0 -1> | 187.0 |
C (mp-66) | <1 1 0> | <1 1 0> | 162.8 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 98.2 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 261.9 |
GdScO3 (mp-5690) | <1 1 1> | <0 0 1> | 294.5 |
Mg (mp-153) | <0 0 1> | <1 0 -1> | 280.5 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 261.9 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 294.5 |
LaF3 (mp-905) | <0 0 1> | <1 0 -1> | 93.5 |
LaF3 (mp-905) | <1 0 0> | <1 0 1> | 160.5 |
LaF3 (mp-905) | <1 0 1> | <1 0 -1> | 280.5 |
LaF3 (mp-905) | <1 1 0> | <1 0 -1> | 93.5 |
PbS (mp-21276) | <1 1 1> | <1 0 -1> | 187.0 |
InP (mp-20351) | <1 1 1> | <1 0 -1> | 187.0 |
TbScO3 (mp-31119) | <1 1 1> | <0 0 1> | 294.5 |
MoSe2 (mp-1634) | <0 0 1> | <1 1 0> | 162.8 |
WS2 (mp-224) | <0 0 1> | <1 0 -1> | 280.5 |
C (mp-48) | <0 0 1> | <0 0 1> | 294.5 |
C (mp-48) | <1 0 0> | <1 0 0> | 174.6 |
C (mp-48) | <1 0 1> | <1 0 0> | 261.9 |
WSe2 (mp-1821) | <0 0 1> | <1 1 0> | 162.8 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <1 0 -1> | 187.0 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 -1> | 280.5 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 87.3 |
ZnO (mp-2133) | <1 0 0> | <1 0 -1> | 280.5 |
Cu (mp-30) | <1 0 0> | <1 0 0> | 261.9 |
Cu (mp-30) | <1 1 0> | <1 0 0> | 261.9 |
Al2O3 (mp-1143) | <0 0 1> | <1 0 -1> | 280.5 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 196.4 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 -1> | 280.5 |
ZrO2 (mp-2858) | <1 1 -1> | <0 1 0> | 137.5 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 196.4 |
YAlO3 (mp-3792) | <1 0 0> | <1 0 1> | 160.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
H4N2O3 (mp-707104) | 0.7357 | 0.160 | 3 |
H9CN5Cl2 (mp-759603) | 0.6369 | 0.141 | 4 |
H9C3N3O2 (mp-556151) | 0.7193 | 0.080 | 4 |
SiH17C11N (mp-571097) | 0.6648 | 0.101 | 4 |
CrH18C5(NO)4 (mp-868120) | 0.6492 | 0.171 | 5 |
MoH18C5(NO)4 (mp-868119) | 0.5683 | 0.105 | 5 |
TlH12C4Br4N5 (mp-568282) | 0.7065 | 0.136 | 5 |
MoH17C5(NO)4 (mp-705911) | 0.5598 | 0.176 | 5 |
ZnH8C4(N4Cl)2 (mp-600171) | 0.6891 | 0.049 | 5 |
ZnPH7C2N4O5 (mp-699466) | 0.5174 | 0.018 | 6 |
Li2H12C3SN6O7 (mp-722272) | 0.5837 | 0.001 | 6 |
SnH4C2NO4F (mp-561270) | 0.5451 | 0.054 | 6 |
ZnP2H14C2(NO)6 (mp-757310) | 0.5889 | 0.050 | 6 |
ZnH12C3S4(N3O2)2 (mp-774708) | 0.6170 | 0.043 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: P H C N O F |
Final Energy/Atom-5.9974 eV |
Corrected Energy-304.0843 eV
-304.0843 eV = -299.8705 eV (uncorrected energy) - 4.2137 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)