Final Magnetic Moment1.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.099 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.462 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSbPO4 + P3H30N7O12 + H2O + Sb2O3 + Sb + C |
Band Gap0.035 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 284.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 285.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 217.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 134.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 -1> | 164.7 |
LiF (mp-1138) | <1 1 0> | <0 1 -1> | 164.7 |
BN (mp-984) | <1 0 1> | <1 -1 -1> | 139.8 |
BN (mp-984) | <1 1 0> | <1 1 -1> | 239.4 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 284.1 |
Al (mp-134) | <1 1 0> | <0 1 -1> | 164.7 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 1> | 223.0 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 285.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 94.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 268.5 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 189.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 268.5 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 285.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 285.6 |
SiO2 (mp-6930) | <1 0 0> | <1 -1 -1> | 139.8 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 285.6 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 285.6 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 284.1 |
TiO2 (mp-2657) | <1 0 0> | <1 -1 1> | 262.1 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 284.1 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 268.5 |
YVO4 (mp-19133) | <1 1 1> | <1 0 1> | 245.8 |
Ag (mp-124) | <1 1 0> | <0 1 -1> | 247.0 |
C (mp-66) | <1 1 0> | <1 -1 0> | 235.4 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 134.2 |
GdScO3 (mp-5690) | <0 1 1> | <0 1 0> | 285.6 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 285.6 |
TbScO3 (mp-31119) | <0 0 1> | <0 1 0> | 285.6 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 134.2 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 134.2 |
BaTiO3 (mp-5986) | <0 0 1> | <1 1 -1> | 239.4 |
SiC (mp-11714) | <1 0 0> | <0 1 0> | 285.6 |
MoSe2 (mp-1634) | <0 0 1> | <1 1 0> | 239.0 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 268.5 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 268.5 |
Au (mp-81) | <1 1 0> | <0 1 -1> | 247.0 |
C (mp-48) | <0 0 1> | <0 0 1> | 268.5 |
C (mp-48) | <1 0 1> | <0 1 1> | 223.0 |
WSe2 (mp-1821) | <0 0 1> | <1 1 0> | 239.0 |
YAlO3 (mp-3792) | <0 1 1> | <1 0 1> | 245.8 |
SiC (mp-8062) | <1 0 0> | <0 1 0> | 285.6 |
MgF2 (mp-1249) | <1 0 1> | <1 0 0> | 284.1 |
MgF2 (mp-1249) | <1 1 1> | <0 0 1> | 268.5 |
ZnO (mp-2133) | <1 1 1> | <0 1 0> | 285.6 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 0> | 285.6 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 134.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2Cr2O7 (mp-771466) | 0.7023 | 0.074 | 3 |
Li3V5O14 (mp-770775) | 0.7498 | 0.096 | 3 |
Sb6S2O15 (mp-27229) | 0.6285 | 0.000 | 3 |
Cr2(Bi2O5)3 (mp-542196) | 0.7201 | 0.000 | 3 |
PH8N3O2 (mp-697683) | 0.7478 | 0.000 | 4 |
PH6N3O (mp-706979) | 0.7107 | 0.007 | 4 |
Al6H16C5(Cl2O)6 (mp-775365) | 0.7337 | 0.072 | 5 |
V3H6CNO7 (mp-600514) | 0.7023 | 0.241 | 5 |
MnP3H10C3NO9 (mp-743546) | 0.6842 | 0.113 | 6 |
Zn3P3H10C2NO13 (mp-709326) | 0.7426 | 0.250 | 6 |
RbLiH4S2(NO3)2 (mp-699447) | 0.7476 | 0.053 | 6 |
NaPH3C2N3O4 (mp-696990) | 0.7382 | 0.411 | 6 |
VH8C2N2O6F (mp-745044) | 0.7272 | 0.088 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sb P H C N O |
Final Energy/Atom-5.7631 eV |
Corrected Energy-277.7434 eV
-277.7434 eV = -265.1022 eV (uncorrected energy) - 12.6412 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)