Final Magnetic Moment23.030 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.528 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.044 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.27 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCo3(AsO4)2 + Co3O4 + Co7(AsO6)2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 -1> | 215.8 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 71.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 322.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 258.2 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 322.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 193.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 183.3 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 292.3 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 305.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 230.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 193.6 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 215.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 -1> | 242.2 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 141.8 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 287.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 64.5 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 193.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 -1> | 287.7 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 215.8 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 322.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 206.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 258.2 |
CdS (mp-672) | <1 0 1> | <1 0 -1> | 287.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 244.3 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 322.7 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 193.6 |
BN (mp-984) | <0 0 1> | <1 0 0> | 244.3 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 287.7 |
BN (mp-984) | <1 1 1> | <0 1 1> | 233.7 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 322.7 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 305.4 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 322.7 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 193.6 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 193.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 258.2 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 -1> | 287.7 |
Mg (mp-153) | <1 0 1> | <1 0 -1> | 287.7 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 292.3 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 0> | 292.3 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 1 0> | 292.3 |
GaP (mp-2490) | <1 1 0> | <1 0 -1> | 215.8 |
InP (mp-20351) | <1 0 0> | <1 1 1> | 141.8 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 -1> | 287.7 |
TbScO3 (mp-31119) | <1 0 0> | <1 1 0> | 230.0 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 258.2 |
Ni (mp-23) | <1 1 0> | <1 0 1> | 103.1 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 193.6 |
PbSe (mp-2201) | <1 1 0> | <1 0 -1> | 215.8 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 -1> | 143.9 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 258.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ni17(As3O16)2 (mp-764249) | 0.1800 | 0.005 | 3 |
Ni17(As3O16)2 (mp-705872) | 0.1860 | 0.000 | 3 |
Mg17(As3O16)2 (mp-757303) | 0.1598 | 0.000 | 3 |
Mg17(As3O16)2 (mp-531778) | 0.1692 | 0.025 | 3 |
Co7(AsO6)2 (mp-24892) | 0.5005 | 0.000 | 3 |
Li3Mn8(OF3)4 (mp-763504) | 0.2931 | 0.072 | 4 |
Li3Fe9O5F11 (mp-850170) | 0.4444 | 0.076 | 4 |
Li3Fe8O3F13 (mp-764637) | 0.3380 | 0.071 | 4 |
Li3Ni8(OF3)4 (mp-765304) | 0.3486 | 0.076 | 4 |
Co8Te(AsO8)2 (mp-699598) | 0.4851 | 0.023 | 4 |
Al2O3 (mp-752826) | 0.6768 | 0.079 | 2 |
Al2O3 (mp-685036) | 0.6538 | 0.111 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Co As O |
Final Energy/Atom-6.1125 eV |
Corrected Energy-191.2655 eV
-191.2655 eV = -165.0369 eV (uncorrected energy) - 14.9920 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)