Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.140 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.125 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.33 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMoCl5 + SCl2O |
Band Gap1.832 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 122.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 287.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 287.4 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 191.6 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 122.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 287.4 |
BN (mp-984) | <1 1 1> | <0 1 0> | 233.8 |
GaN (mp-804) | <1 0 0> | <1 1 -1> | 167.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 287.4 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 245.5 |
Al (mp-134) | <1 1 1> | <0 0 1> | 287.4 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 184.7 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 233.8 |
C (mp-66) | <1 1 0> | <0 0 1> | 287.4 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 287.4 |
InSb (mp-20012) | <1 1 0> | <1 0 1> | 184.7 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 95.8 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 287.4 |
ZrO2 (mp-2858) | <0 1 0> | <1 1 0> | 169.5 |
SiC (mp-8062) | <1 1 0> | <1 0 0> | 245.5 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 95.8 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 287.4 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 287.4 |
TiO2 (mp-390) | <1 0 0> | <1 0 1> | 184.7 |
MgF2 (mp-1249) | <1 1 0> | <1 0 1> | 184.7 |
Al2O3 (mp-1143) | <1 0 0> | <1 0 0> | 122.7 |
LiAlO2 (mp-3427) | <1 0 0> | <0 1 0> | 233.8 |
Fe2O3 (mp-24972) | <1 0 1> | <0 0 1> | 287.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Re2Cl7O3 (mp-672376) | 0.6576 | 0.000 | 3 |
NaBrO3 (mp-608595) | 0.6702 | 0.517 | 3 |
K2Mo4O13 (mp-561805) | 0.6575 | 0.010 | 3 |
TcO3F (mp-555390) | 0.5582 | 0.021 | 3 |
Hg2Mo5O16 (mp-505304) | 0.6553 | 0.019 | 3 |
KXeO3F (mp-554762) | 0.6639 | 0.547 | 4 |
K2Mo(I2O7)2 (mp-558187) | 0.6425 | 0.000 | 4 |
ReNCl4O3 (mp-647116) | 0.5962 | 0.004 | 4 |
BaMoSeO6 (mp-566189) | 0.6348 | 0.013 | 4 |
K2MoSeO6 (mp-566249) | 0.6746 | 0.000 | 4 |
OF3 (mp-974002) | 0.6924 | 0.207 | 2 |
XeO3 (mp-562054) | 0.6830 | 0.945 | 2 |
B5H7 (mp-706630) | 0.7289 | 0.000 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMo: 4.38 eV |
PseudopotentialsVASP PAW: Mo_pv S Cl O |
Final Energy/Atom-3.5214 eV |
Corrected Energy-160.4430 eV
-160.4430 eV = -140.8560 eV (uncorrected energy) - 14.1240 eV (MP Advanced Correction) - 5.4630 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)