Final Magnetic Moment1.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.349 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.106 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.32 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSi2Pb3O7 + SiPbO3 + Mn2SiO4 |
Band Gap3.245 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3c [167] |
Hall-R 3 2"c |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
InAs (mp-20305) | <1 1 1> | <0 0 1> | 268.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 268.9 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 268.9 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 268.9 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 89.6 |
BN (mp-984) | <1 1 0> | <0 0 1> | 268.9 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 268.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 268.9 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 268.9 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 268.9 |
C (mp-66) | <1 1 1> | <0 0 1> | 89.6 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 268.9 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 268.9 |
Au (mp-81) | <1 1 1> | <0 0 1> | 89.6 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 89.6 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 89.6 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 89.6 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 268.9 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 268.9 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 268.9 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 268.9 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 268.9 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 268.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaPO3 (mp-864891) | 0.7157 | 0.002 | 3 |
La2(SiO3)3 (mp-756888) | 0.6963 | 0.029 | 3 |
Ge3Pb5O11 (mp-557340) | 0.5112 | 0.010 | 3 |
Ge3Pb5O11 (mp-557667) | 0.5494 | 0.012 | 3 |
Cd(PO3)2 (mp-4659) | 0.7156 | 0.000 | 3 |
Li7Cr2P7O24 (mp-773702) | 0.6251 | 0.106 | 4 |
Li2Co3(P2O7)2 (mp-585195) | 0.6347 | 0.049 | 4 |
Li2Co3(P2O7)2 (mp-540469) | 0.6331 | 0.049 | 4 |
Li2Mn3(P2O7)2 (mp-31933) | 0.6083 | 0.030 | 4 |
LiV3P3O11 (mp-763468) | 0.6410 | 0.080 | 4 |
MnFeCo(PO4)3 (mp-764410) | 0.7432 | 0.027 | 5 |
KNaZnP2O7 (mp-554157) | 0.6955 | 0.000 | 5 |
NaInBP2HO9 (mp-757312) | 0.7419 | 0.013 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Mn_pv Si Pb_d O |
Final Energy/Atom-6.7625 eV |
Corrected Energy-519.7584 eV
-519.7584 eV = -486.9005 eV (uncorrected energy) - 29.4962 eV (MP Anion Correction) - 3.3617 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)