Final Magnetic Moment1.040 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.288 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.661 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 137.2 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 141.6 |
BN (mp-984) | <0 0 1> | <0 1 1> | 197.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 137.2 |
BN (mp-984) | <1 1 0> | <0 1 0> | 137.2 |
BN (mp-984) | <1 1 1> | <0 1 0> | 137.2 |
PbSe (mp-2201) | <1 1 1> | <0 1 0> | 137.2 |
C (mp-48) | <0 0 1> | <0 1 0> | 137.2 |
C (mp-48) | <1 1 1> | <0 1 0> | 137.2 |
CdSe (mp-2691) | <1 1 1> | <0 1 0> | 137.2 |
GaSb (mp-1156) | <1 1 1> | <0 1 0> | 137.2 |
Cu (mp-30) | <1 1 1> | <0 1 0> | 137.2 |
Fe2O3 (mp-24972) | <0 0 1> | <0 1 0> | 137.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Bi6P2O15 (mp-767410) | 0.6341 | 0.072 | 3 |
P2Pb4O9 (mp-31068) | 0.6277 | 0.000 | 3 |
Cd2P2O7 (mp-27686) | 0.6098 | 0.000 | 3 |
Bi3(PO5)2 (mp-584116) | 0.5979 | 0.082 | 3 |
Cd3(PO4)2 (mp-680761) | 0.6473 | 0.000 | 3 |
Li3Bi(PO4)2 (mp-778460) | 0.5576 | 0.056 | 4 |
Na4MoS3O14 (mp-565395) | 0.5637 | 0.000 | 4 |
K4Zn(WO4)3 (mp-622489) | 0.5188 | 0.020 | 4 |
K4Mn(MoO4)3 (mp-566918) | 0.5097 | 0.116 | 4 |
V2Zn(PO4)2 (mvc-10167) | 0.5627 | 0.075 | 4 |
SrCaTi(PO4)2 (mvc-2770) | 0.6346 | 0.149 | 5 |
SrMgNi(PO4)2 (mvc-2996) | 0.6185 | 0.019 | 5 |
SrCaCo(PO4)2 (mvc-3004) | 0.6082 | 0.027 | 5 |
SrMgFe(PO4)2 (mvc-3019) | 0.6689 | 0.015 | 5 |
SrCaFe(PO4)2 (mvc-3052) | 0.5964 | 0.017 | 5 |
Li3VCrP2(HO5)2 (mp-767626) | 0.7354 | 0.068 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Na_pv V_pv S O |
Final Energy/Atom-6.0147 eV |
Corrected Energy-1107.5911 eV
Uncorrected energy = -1010.4711 eV
Composition-based energy adjustment (-0.503 eV/atom x 24.0 atoms) = -12.0720 eV
Composition-based energy adjustment (-0.687 eV/atom x 104.0 atoms) = -71.4480 eV
Composition-based energy adjustment (-1.700 eV/atom x 8.0 atoms) = -13.6000 eV
Corrected energy = -1107.5911 eV
|