material

SiO2

ID:

mp-7000

DOI:

10.17188/1272685


Tags: Quartz high Quartz alpha Quartz low Silicon oxide High pressure experimental phase Quartz

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-3.257 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.011 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.49 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
SiO2
Band Gap
5.678 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3121 [152]
Hall
P 31 2"
Point Group
32
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 27745 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.000 21.8
SiO2 (mp-6930) <1 0 0> <1 0 0> 0.000 27.7
SiO2 (mp-6930) <1 1 0> <1 1 0> 0.000 47.9
SiO2 (mp-6930) <1 1 1> <1 1 1> 0.000 52.7
SiO2 (mp-6930) <1 0 1> <1 0 1> 0.000 35.3
ZnO (mp-2133) <0 0 1> <0 0 1> 0.000 65.5
BN (mp-984) <0 0 1> <0 0 1> 0.000 21.8
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.000 283.9
KCl (mp-23193) <1 1 1> <0 0 1> 0.001 283.9
Ge3(BiO3)4 (mp-23560) <1 1 1> <0 0 1> 0.001 196.5
GdScO3 (mp-5690) <0 1 0> <1 0 0> 0.001 221.4
GdScO3 (mp-5690) <0 0 1> <1 1 0> 0.002 95.9
MgO (mp-1265) <1 1 1> <0 0 1> 0.004 283.9
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.006 196.5
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.008 283.9
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.010 262.0
LiF (mp-1138) <1 1 1> <0 0 1> 0.010 87.3
GaN (mp-804) <1 0 0> <1 0 0> 0.011 304.4
Mg (mp-153) <1 1 0> <1 1 0> 0.013 143.8
WSe2 (mp-1821) <1 0 0> <1 0 0> 0.014 249.0
AlN (mp-661) <1 0 0> <1 0 0> 0.015 110.7
InAs (mp-20305) <1 1 1> <0 0 1> 0.017 65.5
Ge (mp-32) <1 1 0> <1 0 1> 0.018 141.0
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.020 65.5
GaSe (mp-1943) <0 0 1> <0 0 1> 0.021 87.3
SiC (mp-8062) <1 0 0> <0 0 1> 0.023 152.9
MgAl2O4 (mp-3536) <1 1 0> <1 0 1> 0.023 282.0
GaAs (mp-2534) <1 1 0> <1 0 1> 0.023 141.0
YAlO3 (mp-3792) <1 1 1> <1 0 0> 0.023 249.0
TbScO3 (mp-31119) <0 1 0> <1 0 0> 0.024 221.4
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.024 21.8
C (mp-66) <1 1 1> <0 0 1> 0.029 21.8
ZrO2 (mp-2858) <0 1 1> <0 0 1> 0.029 196.5
CdS (mp-672) <0 0 1> <0 0 1> 0.029 196.5
ZnSe (mp-1190) <1 1 0> <1 0 1> 0.030 141.0
BaTiO3 (mp-5986) <1 0 1> <1 1 1> 0.030 210.7
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.031 95.9
Si (mp-149) <1 0 0> <1 1 0> 0.031 239.6
CeO2 (mp-20194) <1 0 0> <1 1 0> 0.031 239.6
Te2W (mp-22693) <0 0 1> <1 0 1> 0.032 176.3
CaCO3 (mp-3953) <1 0 0> <0 0 1> 0.036 87.3
CaCO3 (mp-3953) <1 1 1> <0 0 1> 0.037 152.9
ZnO (mp-2133) <1 1 1> <1 0 0> 0.039 221.4
AlN (mp-661) <1 0 1> <1 0 0> 0.039 249.0
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.041 152.9
Te2W (mp-22693) <0 1 1> <1 1 0> 0.043 287.6
Si (mp-149) <1 1 1> <0 0 1> 0.044 152.9
GaN (mp-804) <1 1 0> <1 1 0> 0.051 143.8
CdWO4 (mp-19387) <1 0 0> <1 0 1> 0.052 246.8
DyScO3 (mp-31120) <0 1 0> <1 0 0> 0.052 221.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
82 -7 6 15 0 0
-7 82 6 -15 0 0
6 6 86 0 0 0
15 -15 0 52 0 0
0 0 0 0 52 15
0 0 0 0 15 44
Compliance Tensor Sij (10-12Pa-1)
12.9 0.4 -1.0 -3.7 0.0 0.0
0.4 12.9 -1.0 3.7 -0.0 0.0
-1.0 -1.0 11.8 0.0 -0.0 -0.0
-3.7 3.7 0.0 21.5 0.0 -0.0
0.0 -0.0 -0.0 0.0 21.5 -7.5
0.0 0.0 -0.0 -0.0 -7.5 25.1
Shear Modulus GV
46 GPa
Bulk Modulus KV
29 GPa
Shear Modulus GR
42 GPa
Bulk Modulus KR
29 GPa
Shear Modulus GVRH
44 GPa
Bulk Modulus KVRH
29 GPa
Elastic Anisotropy
0.54
Poisson's Ratio
-0.00

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.13684 -0.13683 0.00000 -0.00972 0.00000 0.00000
0.00000 0.00000 0.00000 0.00000 0.00972 -0.13683
0.00000 0.00000 0.00000 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
0.19376 C/m2
Crystallographic Direction vmax
-1.00000
0.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
2.41 -0.00 0.00
-0.00 2.41 0.00
0.00 0.00 2.44
Dielectric Tensor εij (total)
4.51 -0.00 -0.00
-0.00 4.51 0.00
-0.00 0.00 4.74
Polycrystalline dielectric constant εpoly
(electronic contribution)
2.42
Polycrystalline dielectric constant εpoly
(total)
4.59
Refractive Index n
1.56
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
AlPO4 (mp-7848) 0.2751 0.000 3
AlPO4 (mp-3955) 0.2650 0.009 3
AlPO4 (mp-4051) 0.2843 0.002 3
BePO4 (mp-760410) 0.1406 0.064 3
AlPO4 (mp-5331) 0.2655 0.009 3
CsBeAsO4 (mp-9113) 0.7479 0.000 4
Cs2MgSi5O12 (mp-1019610) 0.7376 0.000 4
WN2 (mp-754629) 0.0934 0.102 2
TiO2 (mp-553432) 0.1079 0.049 2
SiO2 (mp-12787) 0.1168 0.010 2
BeF2 (mp-15951) 0.0933 0.000 2
SiO2 (mp-6930) 0.0091 0.010 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

Sol-gel TiO2-SiO2 films were deposited on 316L stainless steel by dip coating process from a sono-catalysed sol of composition 30TiO2-70SiO2 prepared from a mixture of Ti(OC2H5)4 and Si(OC2H5)4, absol [...]
Bisphenol A polycarbonate (Makrolon RX 1805) from Bayer MaterialScience AG (Germany) was used as polymer matrix. A type of hydrophobic nano-SiO2 (Aerosil R8200) was chosen as filler, which was supplie [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition SiO2.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Si O
Final Energy/Atom
-7.9057 eV
Corrected Energy
-75.2732 eV
Uncorrected energy = -71.1512 eV Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV Corrected energy = -75.2732 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 79634
  • 201354
  • 200726
  • 201353
  • 39830
  • 67125
  • 200727
  • 89660
  • 79637
  • 79635
  • 200725
  • 247141
  • 154289
  • 89658
  • 79636
  • 200728
  • 89659
  • 89661
  • 67117
  • 201352
  • 67124
  • 67122
  • 67123
  • 200724
  • 67126
  • 200721
  • 200729
  • 27745
  • 31048
  • 93974
  • 40009
  • 29122
  • 74529
  • 67121
  • 200722
  • 90145
  • 200723
Submitted by
User remarks:
  • Quartz low
  • Silicon oxide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)