Final Magnetic Moment6.006 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.496 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.28 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.453 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP41212 [92] |
HallP 4abw 2nw |
Point Group422 |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 249.0 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 249.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 166.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 83.0 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 173.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 166.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 83.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 83.0 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 173.7 |
Al (mp-134) | <1 0 0> | <0 0 1> | 83.0 |
CdTe (mp-406) | <1 0 0> | <1 0 1> | 173.7 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 249.0 |
LiTaO3 (mp-3666) | <1 1 0> | <0 0 1> | 249.0 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 166.0 |
TiO2 (mp-2657) | <0 0 1> | <1 0 1> | 173.7 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 83.0 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 152.6 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 249.0 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <0 0 1> | 166.0 |
C (mp-66) | <1 0 0> | <0 0 1> | 166.0 |
MgF2 (mp-1249) | <1 0 0> | <1 0 1> | 173.7 |
MgF2 (mp-1249) | <1 1 1> | <0 0 1> | 249.0 |
InSb (mp-20012) | <1 0 0> | <1 0 1> | 173.7 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 249.0 |
Ge (mp-32) | <1 0 0> | <0 0 1> | 166.0 |
Fe2O3 (mp-24972) | <1 1 0> | <0 0 1> | 249.0 |
Fe2O3 (mp-24972) | <1 1 1> | <0 0 1> | 249.0 |
Au (mp-81) | <1 0 0> | <1 0 1> | 173.7 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 166.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnSiO3 (mp-699377) | 0.6964 | 0.082 | 3 |
CaGeO3 (mp-554549) | 0.7045 | 0.039 | 3 |
Fe2P4Pb3O16 (mp-704946) | 0.1686 | 0.149 | 4 |
CaSb2(PO5)2 (mvc-8692) | 0.5548 | 0.125 | 4 |
CaP2(WO5)2 (mvc-9143) | 0.5396 | 0.048 | 4 |
CaMo2(PO5)2 (mvc-9150) | 0.5722 | 0.061 | 4 |
CaMn3(P2O7)2 (mvc-942) | 0.5903 | 0.006 | 4 |
Na3Ca10Mn7V12O48 (mp-694988) | 0.7439 | 0.207 | 5 |
Li3MnV(PO4)3 (mp-779826) | 0.6994 | 0.142 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Cr_pv P Pb_d O |
Final Energy/Atom-7.1362 eV |
Corrected Energy-774.6694 eV
-774.6694 eV = -713.6189 eV (uncorrected energy) - 44.9466 eV (MP Anion Correction) - 16.1040 eV (MP Advanced Correction)
|