Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.635 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.09 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.565 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 223.5 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 223.5 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 223.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 223.5 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 149.0 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 223.5 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 74.5 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 154.9 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 223.5 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 263.9 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 217.8 |
C (mp-66) | <1 0 0> | <0 0 1> | 153.2 |
C (mp-66) | <1 1 0> | <0 1 0> | 108.9 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 223.5 |
Mg (mp-153) | <1 0 1> | <0 1 1> | 187.9 |
KP(HO2)2 (mp-23959) | <1 1 1> | <1 0 0> | 149.0 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 149.0 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 223.5 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 149.0 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 223.5 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 298.0 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 223.5 |
SiC (mp-11714) | <1 0 0> | <1 0 -1> | 154.9 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 153.2 |
Au (mp-81) | <1 1 0> | <1 0 0> | 74.5 |
C (mp-48) | <1 0 0> | <1 0 -1> | 154.9 |
WSe2 (mp-1821) | <1 0 0> | <1 0 0> | 149.0 |
ZrO2 (mp-2858) | <1 1 -1> | <1 0 0> | 223.5 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 223.5 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <1 0 0> | 149.0 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 223.5 |
SiC (mp-8062) | <1 1 0> | <1 0 0> | 298.0 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 1> | 184.4 |
CdWO4 (mp-19387) | <0 1 0> | <1 1 0> | 132.0 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 223.5 |
MgF2 (mp-1249) | <1 0 0> | <0 1 0> | 217.8 |
MgF2 (mp-1249) | <1 1 0> | <1 0 0> | 223.5 |
Cu (mp-30) | <1 1 0> | <1 0 0> | 74.5 |
Al2O3 (mp-1143) | <0 0 1> | <1 0 0> | 298.0 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 0> | 223.5 |
Fe2O3 (mp-24972) | <0 0 1> | <1 0 1> | 184.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCr2F12 (mvc-12792) | 0.3806 | 0.005 | 3 |
V3OF11 (mp-764113) | 0.3481 | 0.126 | 3 |
MnSb2F12 (mp-555052) | 0.3611 | 0.000 | 3 |
V3OF11 (mp-781011) | 0.3439 | 0.126 | 3 |
MnSb2F12 (mp-629044) | 0.3601 | 0.000 | 3 |
MgSb2H2F14 (mp-849311) | 0.5695 | 0.000 | 4 |
CuSb2(XeF8)2 (mp-606617) | 0.5869 | 0.000 | 4 |
Sb2SNF11 (mp-560450) | 0.5228 | 0.067 | 4 |
Te6Mo(OF5)6 (mp-556854) | 0.4686 | 0.014 | 4 |
ReTe5O6F25 (mp-649177) | 0.5248 | 0.026 | 4 |
MnF4 (mp-705480) | 0.2796 | 0.192 | 2 |
VF4 (mp-765919) | 0.3299 | 0.013 | 2 |
VF4 (mp-611846) | 0.3325 | 0.000 | 2 |
VF4 (mp-554799) | 0.3185 | 0.000 | 2 |
Mn2F7 (mp-765268) | 0.3364 | 0.342 | 2 |
CoSb2S2(OF3)4 (mp-629319) | 0.6558 | 0.001 | 5 |
HgSb4C2(OF11)2 (mp-556903) | 0.6060 | 0.080 | 5 |
Sb2OsC4(OF3)4 (mp-559010) | 0.6582 | 0.057 | 5 |
Sb4RuC6(O3F11)2 (mp-555952) | 0.6912 | 0.092 | 5 |
MnAs2S2(OF3)4 (mp-562665) | 0.6909 | 0.040 | 5 |
Sb4IrC5ClO5F22 (mp-555612) | 0.7466 | 0.108 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Cr_pv F |
Final Energy/Atom-5.2990 eV |
Corrected Energy-228.0629 eV
-228.0629 eV = -211.9589 eV (uncorrected energy) - 16.1040 eV (MP Advanced Correction)
|