Final Magnetic Moment0.024 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.062 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.242 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.07 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiNi2P3O10 + Li4P2O7 + LiNiPO4 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2 [5] |
HallC 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 130.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 260.0 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 260.0 |
GaP (mp-2490) | <1 1 0> | <1 0 0> | 130.0 |
NdGaO3 (mp-3196) | <0 1 1> | <1 0 0> | 260.0 |
NdGaO3 (mp-3196) | <0 1 0> | <1 0 0> | 130.0 |
MoSe2 (mp-1634) | <1 0 1> | <1 0 0> | 260.0 |
Si (mp-149) | <1 1 0> | <1 0 0> | 130.0 |
C (mp-48) | <0 0 1> | <1 1 0> | 190.2 |
WSe2 (mp-1821) | <1 0 1> | <1 0 0> | 260.0 |
TiO2 (mp-390) | <1 1 0> | <1 0 0> | 260.0 |
TiO2 (mp-390) | <1 0 0> | <1 0 0> | 260.0 |
CsI (mp-614603) | <1 1 0> | <1 0 0> | 260.0 |
ZnO (mp-2133) | <1 0 0> | <1 0 0> | 260.0 |
SrTiO3 (mp-4651) | <1 0 0> | <1 0 0> | 130.0 |
Al2O3 (mp-1143) | <1 0 0> | <1 0 0> | 130.0 |
CaF2 (mp-2741) | <1 1 0> | <1 0 0> | 130.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3V5O12 (mp-777032) | 0.5613 | 0.133 | 3 |
PRhO4 (mp-28870) | 0.6165 | 0.000 | 3 |
CoSiO3 (mp-699575) | 0.6079 | 0.020 | 3 |
FeAsO4 (mp-19398) | 0.5855 | 0.000 | 3 |
MgSiO3 (mp-1020115) | 0.6142 | 0.031 | 3 |
Li3Fe2(PO4)3 (mp-773942) | 0.4102 | 0.071 | 4 |
Li2Mo(PO4)2 (mp-540296) | 0.3952 | 0.063 | 4 |
Li3Cr2(PO4)3 (mp-31681) | 0.1333 | 0.042 | 4 |
Li3Ti2(PO4)3 (mp-758310) | 0.4054 | 0.075 | 4 |
Li3Ni2(PO4)3 (mp-704207) | 0.3241 | 0.242 | 4 |
MoO2 (mvc-6944) | 0.6816 | 0.387 | 2 |
Li3MnV(PO4)3 (mp-774954) | 0.4277 | 0.241 | 5 |
Li3MnV(PO4)3 (mp-774311) | 0.3751 | 0.208 | 5 |
Li3MnV(PO4)3 (mp-779860) | 0.4303 | 0.272 | 5 |
Li3MnV(PO4)3 (mp-779802) | 0.4276 | 0.173 | 5 |
LiFePO4F (mp-771908) | 0.4593 | 0.037 | 5 |
Li4TiNi3Sn2(PO4)6 (mp-778249) | 0.6619 | 0.173 | 6 |
NaLi5Ti3Cr3(PO4)9 (mp-744549) | 0.7136 | 0.059 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.6623 | 0.003 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.4966 | 0.041 | 6 |
Mn4Si4SnB2(HO9)2 (mp-743890) | 0.6761 | 0.000 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6212 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ni_pv P O |
Final Energy/Atom-6.0697 eV |
Corrected Energy-536.5995 eV
-536.5995 eV = -485.5776 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction) - 17.3120 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)