Final Magnetic Moment0.985 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.224 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.100 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.83 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiPO3 + LiNi2P3O10 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 -1> | 221.3 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 -1> | 236.8 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 128.4 |
AlN (mp-661) | <0 0 1> | <1 1 -1> | 118.4 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 79.7 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 126.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 135.4 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 239.2 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 128.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 203.1 |
GaAs (mp-2534) | <1 1 0> | <1 1 -1> | 236.8 |
GaAs (mp-2534) | <1 1 1> | <1 1 -1> | 118.4 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 295.1 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 295.1 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 172.9 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 239.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 -1> | 236.8 |
ZnSe (mp-1190) | <1 1 1> | <1 1 -1> | 118.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 177.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 252.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 319.0 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 172.9 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 252.9 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 252.9 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 319.0 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 177.9 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 295.1 |
Te2W (mp-22693) | <1 0 1> | <0 1 0> | 210.8 |
YVO4 (mp-19133) | <1 1 0> | <0 1 1> | 319.0 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 172.9 |
TePb (mp-19717) | <1 1 1> | <1 1 -1> | 236.8 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 239.2 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 172.9 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 270.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 203.1 |
BN (mp-984) | <0 0 1> | <0 1 0> | 210.8 |
BN (mp-984) | <1 0 0> | <0 1 0> | 337.2 |
BN (mp-984) | <1 0 1> | <0 1 1> | 79.7 |
BN (mp-984) | <1 1 1> | <1 1 -1> | 236.8 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 210.8 |
MoS2 (mp-1434) | <1 0 0> | <0 1 0> | 210.8 |
Al (mp-134) | <1 1 0> | <0 1 0> | 252.9 |
Al (mp-134) | <1 1 1> | <0 1 1> | 319.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 135.4 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 1> | 159.5 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 168.6 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 -1> | 221.3 |
CdTe (mp-406) | <1 0 0> | <1 0 1> | 172.9 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 128.4 |
CdTe (mp-406) | <1 1 1> | <1 1 -1> | 236.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn2As2O7 (mp-779594) | 0.5621 | 0.000 | 3 |
Mn4(PO4)3 (mp-540071) | 0.6510 | 0.035 | 3 |
Zn2P2O7 (mp-559319) | 0.5626 | 0.000 | 3 |
Li2S2O7 (mp-1020013) | 0.5893 | 0.000 | 3 |
CrCuO4 (mvc-10471) | 0.6115 | 0.066 | 3 |
LiFeP2O7 (mp-762468) | 0.3280 | 0.256 | 4 |
LiCoP2O7 (mp-705301) | 0.3471 | 0.155 | 4 |
LiCrP2O7 (mp-705361) | 0.3355 | 0.190 | 4 |
LiFeP2O7 (mp-695816) | 0.3899 | 0.060 | 4 |
LiMnP2O7 (mp-697744) | 0.3328 | 0.212 | 4 |
BaZn2As3HO11 (mp-758313) | 0.6535 | 0.007 | 5 |
Na2Li2V3P2O13 (mp-853239) | 0.6745 | 0.061 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ni_pv P O |
Final Energy/Atom-6.4119 eV |
Corrected Energy-310.4448 eV
-310.4448 eV = -282.1247 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 8.6560 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)